Endohedral Metallofullerenes
January 18, 2017 – Researchers from Moscow, Leeds, Ulm, San Sebastián and Nottingham have wrapped clusters of 50–70 nickel atoms in carbon cages, creating endohedral metallofullerenes far larger than any made before and with a metal that conventional methods cannot enclose. The 80 kV electron beam of an aberration-corrected TEM both triggered and filmed the reaction inside carbon nanotubes, and molecular dynamics simulations showed why the beam yields six times more caged clusters than heat.
A football-shaped cage of carbon atoms with a metal tucked inside sounds like a curiosity, but such endohedral metallofullerenes (EMFs) could serve as contrast agents, drug carriers or building blocks for molecular electronics. The trouble is making them: only a few metals can be packed into a cage, and only a handful of atoms at a time. An international team from Moscow, Leeds, Ulm, San Sebastián and Nottingham has now built EMFs around clusters of 50–70 nickel atoms, using the electron beam of an image-side Cs-corrected FEI Titan 80-300 transmission electron microscope at 80 kV both to drive the reaction and to film it, with carbon nanotubes as tiny reaction flasks (Fig. 1). Molecular dynamics simulations explain why the beam does a better job than heat.
Metal in a carbon cage
EMFs are fullerenes that hold an extra atom, ion or cluster in their interior. They have great potential for biology, medicine and molecular electronics[1]–[3]. The carbon shell isolates the metal from its surroundings, so an EMF combines high stability with low toxicity, a distinct advantage over the metal chelate complexes commonly used in nuclear medicine and diagnostic radiology.
The traditional routes to EMFs, arc discharge and laser evaporation, are restricted mainly to alkaline earth metals, lanthanides and early transition metals. Modified arc discharge methods have added a select group of small clusters such as metal nitrides and carbides[4],[5]; noble gas atoms have been pushed into finished cages under high pressure[6], and very small molecules such as hydrogen and water have been sealed in through long sequences of organic reactions[7],[8]. Late transition metals such as nickel, however, have never made it into a cage this way, and the largest cluster enclosed so far holds just seven atoms, Sc4O3 in a C80 cage[9].
From graphene to fullerene, now with a metal core
The new method grows out of an earlier discovery by the Group of Electron Microscopy of Materials Science at Ulm University and the School of Chemistry at the University of Nottingham: under the electron beam of an aberration-corrected TEM, a small graphene flake curls up into a fullerene[10]. If a metal cluster is attached to enough carbon, about 100 atoms, the same treatment might wrap the carbon around the metal. Unlike the hot arc or laser plume, where a weakly bound metal cluster simply evaporates, the beam works at room temperature: its electrons are energetic enough to knock out light carbon atoms, but the heavy metal atoms stay where they are.
“When the energy and dose rate of the e-beam are controlled, it is possible to trigger chemical reactions between metal clusters and carbon,” says Prof. Ute Kaiser, head of the SALVE project. “The formation of cage-like structures from amorphous carbon is driven by the energetic requirement of the carbon system to reduce the number of high energy, low coordinate atoms.”
HRTEM imaging reveals the dynamics of metal–carbon bonding, and many metal-catalysed processes driven by the kinetic energy of the beam have already been followed atom by atom[11]–[15]. The open question was how these processes relate to the conditions in a real synthesis. Answering it needs both experiments and simulations under controlled beam and heating conditions.
A central question in studying new low-dimensional materials in metallofullerenes is their structure and the stability of their lattice. Under the high-energy electron beam of a TEM, the protective carbon framework is often seen to collapse[16]: the enclosed metal induces local strain in the lattice and enhances bond breaking by the beam (radiolysis and knock-on damage), so that the cage breaks open or fuses with its neighbours. Research therefore asks how far new hybrid materials can prevent this structural decay[17].
Nickel clusters in nano test tubes
Single-walled carbon nanotubes (SWNTs) make ideal reaction flasks: they are inert, they keep reactants in place, and their walls are only one atom thick, so the microscope can look straight through them. The team filled SWNTs with a nickel complex that breaks down into pure metal and leaves the tubes as small fragments. The nickel atoms gather into clusters of 50–100 atoms that sit in close contact with the inner wall (Fig. 2a), and X-ray spectroscopy confirmed that they are nickel (Fig. 2b). How the tubes were filled is described in a box below.
Carbon cages grow around the metal
Under the 80 keV beam, the amorphous carbon around each nickel cluster rearranged into curved shells. Image simulations of nickel–carbon models confirmed that these shells are carbon; how the images were recorded and simulated is described in a box below. Some shells grew out of a large cluster like a short, open-ended nanotube, with the nickel cluster built into the carbon framework as a patch: a so-called patched heterofullerene (Fig. 2c, Video 1). Others closed completely around the cluster (Fig. 2d,e, Videos 2 and 3). How these images were taken and simulated is shown in the box below (Fig. 3).
Video 1: AC-HRTEM time series at 80 kV: a nickel cluster reacts with the nanotube wall and extrudes a carbon cage while becoming part of it, a patched fullerene (Supporting Video 1 of the paper).
Video 2: AC-HRTEM time series at 80 kV in a nanotube with a wall defect: the nickel cluster first reacts with the defect, then a carbon cage encases it completely (Supporting Video 2).
Video 3: AC-HRTEM time series at 80 kV: a carbon cage fully encases a nickel cluster, which passivates the nickel (Supporting Video 3).
The time series show the nickel clusters acting as a stable surface on which the carbon cages evolve, and as a source of dissolved carbon atoms from which they grow. At first the cluster sits in the cage wall as a patch; then the cage slowly closes over it, with the cluster acting as a template, until the metal is completely encased. Once that has happened, the enclosed nickel is passivated and no longer reacts with the nanotube walls.
Whether a cluster ends up inside a cage depends on two things: there must be enough carbon to wrap the whole cluster, and enough room in the nanotube for the cage to fit around it. Where the space is too tight, only the patched structure forms. The closed cages measure about 1 nm across. From the empirical relation between fullerene diameter and atom count, they contain 100–200 carbon atoms; since cages up to C2160 are counted as fullerenes and large endohedral cages such as La2C138 are known, these are EMFs.
Simulating the beam atom by atom
The microscope cannot yet reveal every atomic step of the cage formation, so the team turned to molecular dynamics simulations. With the CompuTEM algorithm[19], they followed a nickel cluster surrounded by amorphous carbon in three settings: under the 80 keV beam inside a nanotube, under the beam in vacuum, and heated to 2500 K inside a nanotube.
In all three cases, the amorphous carbon turned into a fullerene cage, and the position of the nickel cluster at the moment the cage closed decided whether an EMF or a patched heterofullerene formed (Fig. 4). Under the beam inside the nanotube, the cage formed within about 1000 s at an accumulated dose of 4 × 109 e−/nm2, in very good agreement with the experiment. The simulated nickel–nickel distance of 2.4 Å, which appears as 2.1 Å in projection, also matches the images. In vacuum, the same structures form (Fig. 5), even more perfectly, because the smaller system allows longer simulation times. Carbon chains hanging from the cage are also typical of simulations of fullerene formation[20].
EMFs proved much more stable than patched heterofullerenes under both the beam and heat: the patched structures tend to turn into closed, empty cages with the cluster stuck to the outside, and the cluster eventually drifts off. EMFs are also more strongly bound (Fig. 6a).
Why the beam beats heat
The simulations also showed how much each setting yields (Fig. 6b). Under the beam inside the nanotube, 36 % of the runs ended as an EMF, compared with 26 % in vacuum and only 6 % with heat alone: the beam gives six times the yield of heat treatment. For patched heterofullerenes the gap is smaller, about 150 %. How often the structures turned into one another, and how their fractions changed over time (Fig. 7), is shown in the box below.
In pure carbon, heat and electron impacts usually lead to the same products. In a metal–carbon system they do not: the beam hands its energy mainly to the light carbon atoms, so it is spent almost entirely on rebuilding the carbon network into a cage. Heat, in contrast, also shakes the nickel cluster, driving it through the forming cage and off it. In addition, the beam knocks out about four carbon atoms per run, and atoms bound to nickel go first, which further favours the closed cage.
The nanotube helps as well. Its wall acts as a very narrow container that stops the cluster from leaving the cage and drifting away, which is why the EMF yield inside the tube is about 40 % higher than in vacuum.
Filling the gap between molecules and nanoparticles
Until now, EMFs made at high temperature in the gas phase by the modified arc discharge method held at most 4–7 atoms[4],[5],[9]. Laser treatment at high temperature, on the other end, produces multi-shell carbon particles with metal cores 5–10 nm across. The new method fills the gap between these two kinds of object, with cages around clusters of up to 50–70 nickel atoms.
It also works by a different mechanism. Both established routes are open systems with an outside supply of carbon. Here the system is isolated, so no extra carbon arrives during the transformation. This shortage of carbon is the main reason why an EMF forms and not a nanotube. And because the heavy metal atoms are not knocked out, their number stays fixed throughout: an EMF made this way contains exactly the cluster that went in.
What it opens up
“This opens up possibilities for volume production of new types of EMFs and heterofullerenes in vacuum or buffer gas,” says Prof. Andrei Khlobystov from the University of Nottingham. “The process is analogous to the graphene flake to fullerene transformation under electron irradiation, which we have observed on graphite surface.”
Methods to make nanometre-sized graphene flakes are being actively developed[21]. Depositing such flakes together with metal clusters on a surface could provide the starting material for EMFs and heterofullerenes made under electron irradiation. The challenge is to stop the forming cages from merging. Since finished EMFs diffuse across a surface more easily than the starting clusters, they could leave the synthesis area on their own, which could be used to separate them.
“With our comprehensive characterization and preparation opportunities we could again shed light on the mechanisms of the carbon shell formation around metal atoms and expand the range of synthesis in nano scale containers,” says Kaiser. “New electronically, optically and magnetically active inorganic nanostructures can possibly be produced in this manner in the future.”
Resource:
Sinitsa, A. S., Chamberlain, T. W., Zoberbier, T., Lebedeva, I. V., Popov, A. M., Knizhnik, A. A., McSweeney, R. L., Biskupek, J., Kaiser, U., Khlobystov, A. N. (2017).
Formation of Nickel Clusters Wrapped in Carbon Cages: Toward New Endohedral Metallofullerene Synthesis.
Nano Lett. 17(2), 1082–1089.
https://doi.org/10.1021/acs.nanolett.6b04607
Download this news article as PDF – for reading on paper, taking notes or filing.
-
Cong, H., Yu, B., Akasaka, T., Lu, X. (2013). Endohedral Metallofullerenes: An Unconventional Core–Shell Coordination Union. Coord. Chem. Rev., 257, 2880–2898. https://doi.org/10.1016/j.ccr.2013.05.020
-
Popov, A. A., Yang, S., Dunsch, L. (2013). Endohedral Fullerenes. Chem. Rev., 113, 5989–6113. https://doi.org/10.1021/cr300297r
-
Yang, S., Wang, C.-R. (2014). Endohedral Fullerenes: From Fundamentals to Applications. World Scientific, Singapore. https://doi.org/10.1142/8785
-
Stevenson, S., Rice, G., Glass, T., Harich, K., Cromer, F., Jordan, M. R., Craft, J., Hadju, E., Bible, R., Olmstead, M. M., Maitra, K., Fisher, A. J., Balch, A. L., Dorn, H. C. (1999). Small-Bandgap Endohedral Metallofullerenes in High Yield and Purity. Nature, 401, 55–57. https://doi.org/10.1038/43415
-
Wang, C.-R., Kai, T., Tomiyama, T., Yoshida, T., Kobayashi, Y., Nishibori, E., Takata, M., Sakata, M., Shinohara, H. (2001). A Scandium Carbide Endohedral Metallofullerene: (Sc2C2)@C84. Angew. Chem. Int. Ed., 40, 397–399. https://doi.org/10.1002/1521-3773(20010119)40:2<397::AID-ANIE397>3.0.CO;2-3
-
Saunders, M., Jiménez-Vázquez, H. A., Cross, R. J., Poreda, R. J. (1993). Stable Compounds of Helium and Neon: He@C60 and Ne@C60. Science, 259, 1428–1430. https://doi.org/10.1126/science.259.5100.1428
-
Komatsu, K., Murata, M., Murata, Y. (2005). Encapsulation of Molecular Hydrogen in Fullerene C60 by Organic Synthesis. Science, 307, 238–240. https://doi.org/10.1126/science.1106185
-
Kurotobi, K., Murata, Y. (2011). A Single Molecule of Water Encapsulated in Fullerene C60. Science, 333, 613–616. https://doi.org/10.1126/science.1206376
-
Mercado, B. Q., Olmstead, M. M., Beavers, C. M., Easterling, M. L., Stevenson, S., Mackey, M. A., Coumbe, C. E., Phillips, J. D., Phillips, J. P., Poblet, J. M., Balch, A. L. (2010). A Seven Atom Cluster in a Carbon Cage, the Crystallographically Determined Structure of Sc4(μ3-O)3@Ih-C80. Chem. Commun., 46, 279–281. https://doi.org/10.1039/B918731F
-
Chuvilin, A., Kaiser, U., Bichoutskaia, E., Besley, N. A., Khlobystov, A. N. (2010). Direct Transformation of Graphene to Fullerene. Nat. Chem., 2, 450–453. https://doi.org/10.1038/nchem.644
-
Helveg, S., López-Cartes, C., Sehested, J., Hansen, P. L., Clausen, B. S., Rostrup-Nielsen, J. R., Abild-Pedersen, F., Nørskov, J. K. (2004). Atomic-Scale Imaging of Carbon Nanofibre Growth. Nature, 427, 426–429. https://doi.org/10.1038/nature02278
-
Chamberlain, T. W., Meyer, J. C., Biskupek, J., Leschner, J., Santana, A., Besley, N. A., Bichoutskaia, E., Kaiser, U., Khlobystov, A. N. (2011). Reactions of the Inner Surface of Carbon Nanotubes and Nanoprotrusion Processes Imaged at the Atomic Scale. Nat. Chem., 3, 732–737. https://doi.org/10.1038/nchem.1115
-
Zoberbier, T., Chamberlain, T. W., Biskupek, J., Kuganathan, N., Eyhusen, S., Bichoutskaia, E., Kaiser, U., Khlobystov, A. N. (2012). Interactions and Reactions of Transition Metal Clusters With the Interior of Single-Walled Carbon Nanotubes Imaged at the Atomic Scale. J. Am. Chem. Soc., 134, 3073–3079. https://doi.org/10.1021/ja208746z
-
Koshino, M., Niimi, Y., Nakamura, E., Kataura, H., Okazaki, T., Suenaga, K., Iijima, S. (2010). Analysis of the Reactivity and Selectivity of Fullerene Dimerization Reactions at the Atomic Level. Nat. Chem., 2, 117–124. https://doi.org/10.1038/nchem.482
-
Yue, Y., Yuchi, D., Guan, P., Xu, J., Guo, L., Liu, J. (2016). Atomic Scale Observation of Oxygen Delivery During Silver–Oxygen Nanoparticle Catalysed Oxidation of Carbon Nanotubes. Nat. Commun., 7, 12251. https://doi.org/10.1038/ncomms12251
-
SALVE news (2012). Knock-on Damage in Graphene Linked to Lattice Vibrations. salve-project.de, May 07, 2012. https://salve-project.de/newspress/knock-on-damage-in-graphene-linked-to-lattice-vibrations.html
-
Tang, J., Xing, G., Zhao, F., Yuan, H., Zhao, Y. (2007). Modulation of Structural and Electronic Properties of Fullerene and Metallofullerenes by Surface Chemical Modifications. J. Nanosci. Nanotechnol., 7, 1085–1101. https://doi.org/10.1166/jnn.2007.301
-
Biskupek, J., Hartel, P., Haider, M., Kaiser, U. (2012). Effects of Residual Aberrations Explored on Single-Walled Carbon Nanotubes. Ultramicroscopy, 116, 1–7. https://doi.org/10.1016/j.ultramic.2012.03.008
-
Santana, A., Zobelli, A., Kotakoski, J., Chuvilin, A., Bichoutskaia, E. (2013). Inclusion of Radiation Damage Dynamics in High-Resolution Transmission Electron Microscopy Image Simulations: The Example of Graphene. Phys. Rev. B, 87, 094110. https://doi.org/10.1103/PhysRevB.87.094110
-
Irle, S., Zheng, G., Wang, Z., Morokuma, K. (2006). The C60 Formation Puzzle “Solved”: QM/MD Simulations Reveal the Shrinking Hot Giant Road of the Dynamic Fullerene Self-Assembly Mechanism. J. Phys. Chem. B, 110, 14531–14545. https://doi.org/10.1021/jp061173z
-
Bacon, M., Bradley, S. J., Nann, T. (2014). Graphene Quantum Dots. Part. Part. Syst. Charact., 31, 415–428. https://doi.org/10.1002/ppsc.201300252