October 15, 2024 – Researchers from Ulm University and Leiden University (the Netherlands) have studied how grain boundaries in nanocrystalline carbon monolayers change under the electron beam, and how this depends on the beam energy. Using the spherical and chromatic aberration-corrected SALVE microscope, they imaged the layers at 80, 60 and 40 kV. At 60 kV and a high dose rate, the beam removed contamination and reshaped grain boundaries atom by atom without tearing holes into the layer. The findings suggest that grain boundaries could one day be engineered on purpose, for filter membranes or nanoscale circuits.

Observing, manipulating and precisely building structures at the atomic scale opens new possibilities in nanotechnology, provided that every individual atom can be controlled.1–3 Such atom-by-atom studies only became possible with spherical (CS) aberration correctors,4,5 monochromators6–10 and hardware correction of the chromatic (CC) aberration,11,12 which allow imaging at accelerating voltages of 80, 60 and 40 kV and even lower.

Graphene reacts to the beam in several ways. A broad 100 kV beam, above graphene’s knock-on threshold of about 86 kV,13 introduces more and more defects into the monolayer until it turns into a disordered state.14 Graphene’s ability to heal itself, however, can be used to lower the defect density again by thermal treatment.15 A high-dose 80 kV beam has even been shown to turn amorphous carbon into nanocrystalline graphene (NCG).16

Changes as small as single defects can alter a material’s properties considerably. Carbon monolayers with little long-range order, such as NCG or amorphous carbon monolayers, therefore behave very differently from pristine graphene, which can give them new functions.17,18 Seven- and eight-membered carbon rings, for example, make an otherwise pristine carbon monolayer more permeable to protons19,20 while it still blocks larger atoms and molecules. Grain boundaries, the seams where two crystal grains of different orientation meet, consist mainly of five- and seven-membered rings.21 Their sequence depends on the angular mismatch between the neighbouring grains,22 and they have already served as simple circuits for chemical sensing.23

As extended defects, grain boundaries strongly affect the structural,24 chemical25 and electronic26 properties of carbon sheets, and they have been studied extensively in theory and experiment.27,28 Their structure can also change under the electron beam: when enough energy is supplied to overcome the activation barriers, a boundary can move into a more favourable configuration,28,29 and small grains can be absorbed completely into the surrounding lattice.28 In principle, the beam can thus reshape grain boundaries. The catch is that the same beam also damages defective carbon much more easily than pristine graphene; the box below explains why.

▸ Background: how the electron beam damages carbon

In the new study, the team examined NCG monolayers with the CC/CS-corrected SALVE microscope at 80, 60 and 40 kV and at different electron dose rates, the number of electrons per area and second. The aim was to find out whether grain boundaries can be reshaped deliberately, for example to create more seven-membered rings, without holes growing in the layer. How the samples were made, and how images were recorded at extreme dose rates, is described in the second box.

▸ Sample and microscope: from a molecular film to high-dose-rate images

80 kV Experiments
When an area was imaged at high resolution for the first time, it appeared completely covered by contamination that hid the atomic positions. Only through small holes in this layer, 1–3 nm across, could individual carbon atoms or rings be seen, about 0–3 such holes per 3,300 nm2 (Fig. 1a). As imaging continued, the amorphous contamination disappeared and revealed the nanocrystalline material beneath. Because NCG consists of small grains, a large share of the monolayer is grain boundary. With its lower knock-on threshold compared with pristine graphene, holes formed and grew and quickly destroyed the monolayer. No large monolayer region was ever visible at once; the exposed patches rarely exceeded 5 nm in diameter (Fig. 1b).

To learn more about how the samples behave under the beam, the researchers raised the dose rate drastically, which led to two key observations. First, the higher dose rate naturally caused more damage. By moving the beam away from an area as soon as holes began to form, however, the damage could be kept small. This worked because only part of the field of view was illuminated. Despite the higher damage rate, more of the monolayer could thus be revealed than at normal dose rates (Fig. 2).

Second, the exposed monolayer regions became large enough to follow their structure during the experiment. A neural network44,45 separated monolayer from contamination and located the carbon atoms. From these positions the carbon rings were mapped, which showed where the grain boundaries run and what they are made of. Ring statistics compared from frame to frame showed the ratio of pentagons to hexagons falling from 0.28 (Fig. 2b) to 0.20 (Fig. 2c), a sign that the monolayer was moving towards a more graphene-like structure. How the network works, and why the edges of the holes hardly affect these numbers, is explained in the third box.

▸ Analysis: counting carbon rings with a neural network

60 kV Experiments
Hole growth at 80 kV made the monolayer hard to study. To reduce knock-on damage while still removing contamination, the team repeated the experiment at 60 kV. At a moderate dose rate, as in the 80 kV experiments, hole growth almost stopped. Even at high dose rates, holes did not form easily and appeared only after prolonged exposure (Fig. 3). The images also showed that the samples are not pure monolayers: bilayer and few-layer regions can be recognized by their moiré patterns (Fig. 3b). Graphene’s ability to heal itself also helps the monolayer survive:37 carbon can fill small holes, as observed at high dose rates. By moving the beam as soon as damage began, as at 80 kV, the damage could be reduced further, which made nearly damage-free imaging at 60 kV possible.

Under these conditions, the monolayer and its response to the beam could be studied in detail. A high-dose-rate image series was recorded at about 5.5 frames per second and a dose rate of about 6 × 107 e·nm−2·s−1, fast enough to follow grain transformations at atomic resolution (Fig. 4). Fig. 4 shows neural-network overlays for eight of the 2,339 frames, chosen to capture the key stages. At first, three grains of different orientation were separated by a grain boundary and surrounded by contamination (Fig. 4a).

As the contamination was removed, the boundary partly enclosing the centre grain came into view; this grain was smaller than the other two (Figs. 4b–d). The boundary around it first closed and then broke open again. The centre grain was then absorbed by the lower grain and left behind the upper part of its boundary, which produced a long, winding boundary between the two remaining grains (Fig. 4e). As the experiment continued, this boundary straightened considerably (Figs. 4f–h). The pentagon-to-hexagon ratio fell from 0.06 in frame 0 to 0.04 in frame 2,327.

The 60 kV beam supplies enough energy for bond rotations in graphene, and it does so only where it hits the sample. Heat, by contrast, would act on the whole sample in a process similar to Ostwald ripening: grains grow, defects disappear, and the change slows and finally stops once the boundaries are long and straight enough that no configuration is clearly favoured.28 With the beam, spreading or focusing changes the dose rate and the size of the irradiated area within moments. This makes it a tool for steering grain motion by irradiating only the areas that serve a given goal.

40 kV Experiments
In search of a way to remove contamination without substantially changing the grain structure, the team also worked at half the accelerating voltage, 40 kV. At a moderate dose rate of about 106 e·nm−2·s−1 for about one hour, the contamination hardly changed and no holes formed. At 40 kV, however, the dose rate is limited to about 7 × 106 e·nm−2·s−1, because higher values would violate radiation safety regulations; the authors put this at about three orders of magnitude below the value at 80 kV. The effect of the 40 kV beam on the grain structure therefore could not be examined. The researchers speculated that a higher dose rate would remove the contamination at 40 kV as well and reveal the grain boundaries.

The study shows how grain boundaries could be engineered. Irradiating several grains at once usually lets the larger grain swallow the smaller ones, but the curvature of a boundary matters too: irradiating its outward-curved parts makes the corresponding grain shrink. Targeting such spots could, for example, grow boundaries rich in seven-membered rings to make the monolayer more permeable to protons,20 or build circuits from grain boundaries.23 For this, the layer has to start with small grains, because the average grain size inevitably grows during irradiation. So far, neither 80 nor 60 kV can clear large areas of contamination without altering the structure, and at 40 kV the available dose rate is too low. “If this method can be paired with techniques to remove contamination without altering the grain structure,” the authors write, “it could lead to precise engineering of grain boundary structure for applications in filter membranes or nanocircuitry.” Aberration-corrected low-voltage HRTEM at Ulm University made it possible to watch such boundaries rearrange atom by atom, in real time.

Resource:
Leist, C., Makurat, M., Jiao, A., Liu, X., Schneider, G. F. & Kaiser, U. (2025).
Control of grain boundary formation in atomically resolved nanocrystalline carbon monolayers: dependence on electron energy.
Microsc. Microanal., 31(1), ozae101.
https://doi.org/10.1093/mam/ozae101

Download this news article as PDF – for reading on paper, taking notes or filing.

References
  1. Zhao, X., Kotakoski, J., Meyer, J.C., et al. (2017). Engineering and modifying two-dimensional materials by electron beams. MRS Bull., 42, 667–676. https://doi.org/10.1557/mrs.2017.184

  2. Susi, T., Meyer, J.C. & Kotakoski, J. (2017). Manipulating low-dimensional materials down to the level of single atoms with electron irradiation. Ultramicroscopy, 180, 163–172. https://doi.org/10.1016/j.ultramic.2017.03.005

  3. Zhao, X., Dan, J., Chen, J., et al. (2018). Atom‐by‐Atom Fabrication of Monolayer Molybdenum Membranes. Adv. Mater., 30, 1707281. https://doi.org/10.1002/adma.201707281

  4. Haider, M., Uhlemann, S., Schwan, E., et al. (1998). Electron microscopy image enhanced. Nature, 392, 768–769. https://doi.org/10.1038/33823

  5. Batson, P.E., Dellby, N. & Krivanek, O.L. (2002). Sub-ångstrom resolution using aberration corrected electron optics. Nature, 418, 617–620. https://doi.org/10.1038/nature00972

  6. Kujawa, S., Erni, R., Freitag, B., et al. (2006). High resolution TEM at 80 kV acceleration voltage – is approaching 1 ångström possible?. Microsc. Microanal., 12, 1470–1471. https://doi.org/10.1017/S143192760606572X

  7. Dellby, N., Murfitt, M., Krivanek, O.L., et al. (2008). Atomic-resolution STEM at 60 kV primary voltage. Microsc. Microanal., 14, 136–137. https://doi.org/10.1017/S1431927608088399

  8. Bell, D., Kolmykov, D. & Russo, C. (2011). Low-voltage (40 kV) aberration-corrected, monochromated, imaging for carbon nanostructures. Microsc. Microanal., 17, 1490–1491. https://doi.org/10.1017/S1431927611008324

  9. Dellby, N., Bacon, N., Hrncirik, P., et al. (2011). Dedicated STEM for 200 to 40 keV operation. Eur. Phys. J. Appl. Phys., 54, 33505. https://doi.org/10.1051/epjap/2011100429

  10. Kaiser, U., Biskupek, J., Meyer, J., et al. (2011). Transmission electron microscopy at 20kV for imaging and spectroscopy. Ultramicroscopy, 111, 1239–1246. https://doi.org/10.1016/j.ultramic.2011.03.012

  11. Linck, M., Hartel, P., Uhlemann, S., et al. (2016). Chromatic Aberration Correction for Atomic Resolution TEM Imaging from 20 to 80 kV. Phys. Rev. Lett., 117, 076101. https://doi.org/10.1103/PhysRevLett.117.076101

  12. Börrnert, F. & Kaiser, U. (2018). Chromatic- and geometric-aberration-corrected TEM imaging at 80 kV and 20 kV. Phys. Rev. A, 98, 023861. https://doi.org/10.1103/PhysRevA.98.023861

  13. Meyer, J.C., Eder, F., Kurasch, S., et al. (2012). Accurate Measurement of Electron Beam Induced Displacement Cross Sections for Single-Layer Graphene. Phys. Rev. Lett., 108, 196102. https://doi.org/10.1103/PhysRevLett.108.196102

  14. Kotakoski, J., Krasheninnikov, A.V., Kaiser, U., et al. (2011). From Point Defects in Graphene to Two-Dimensional Amorphous Carbon. Phys. Rev. Lett., 106, 105505. https://doi.org/10.1103/PhysRevLett.106.105505

  15. Song, B., Schneider, G.F., Xu, Q., et al. (2011). Atomic-Scale Electron-Beam Sculpting of Near-Defect-Free Graphene Nanostructures. Nano Lett., 11, 2247–2250. https://doi.org/10.1021/nl200369r

  16. Börrnert, F., Avdoshenko, S.M., Bachmatiuk, A., et al. (2012). Amorphous Carbon under 80 kV Electron Irradiation: A Means to Make or Break Graphene. Adv. Mater., 24, 5630–5635. https://doi.org/10.1002/adma.201202173

  17. Turchanin, A., Weber, D., Büenfeld, M., et al. (2011). Conversion of Self-Assembled Monolayers into Nanocrystalline Graphene: Structure and Electric Transport. ACS Nano, 5, 3896–3904. https://doi.org/10.1021/nn200297n

  18. Backes, C., Abdelkader, A.M., Alonso, C., et al. (2020). Production and processing of graphene and related materials. 2D Mater., 7, 022001. https://doi.org/10.1088/2053-1583/ab1e0a

  19. Miao, M., Nardelli, M.B., Wang, Q., et al. (2013). First principles study of the permeability of graphene to hydrogen atoms. Phys. Chem. Chem. Phys., 15, 16132. https://doi.org/10.1039/c3cp52318g

  20. Griffin, E., Mogg, L., Hao, G.P., et al. (2020). Proton and Li-Ion Permeation through Graphene with Eight-Atom-Ring Defects. ACS Nano, 14, 7280–7286. https://doi.org/10.1021/acsnano.0c02496

  21. Carlsson, J.M., Ghiringhelli, L.M. & Fasolino, A. (2011). Theory and hierarchical calculations of the structure and energetics of [0001] tilt grain boundaries in graphene. Phys. Rev. B, 84, 165423. https://doi.org/10.1103/PhysRevB.84.165423

  22. Grantab, R., Shenoy, V.B. & Ruoff, R.S. (2010). Anomalous Strength Characteristics of Tilt Grain Boundaries in Graphene. Science, 330, 946–948. https://doi.org/10.1126/science.1196893

  23. Yasaei, P., Kumar, B., Hantehzadeh, R., et al. (2014). Chemical sensing with switchable transport channels in graphene grain boundaries. Nat. Commun., 5, 4911. https://doi.org/10.1038/ncomms5911

  24. Liu, Y. & Yakobson, B.I. (2010). Cones, Pringles, and Grain Boundary Landscapes in Graphene Topology. Nano Lett., 10, 2178–2183. https://doi.org/10.1021/nl100988r

  25. Malola, S., Häkkinen, H. & Koskinen, P. (2010). Structural, chemical, and dynamical trends in graphene grain boundaries. Phys. Rev. B, 81, 165447. https://doi.org/10.1103/PhysRevB.81.165447

  26. Allen, M.J., Tung, V.C. & Kaner, R.B. (2010). Honeycomb Carbon: A Review of Graphene. Chem. Rev., 110, 132–145. https://doi.org/10.1021/cr900070d

  27. Ophus, C., Shekhawat, A., Rasool, H., et al. (2015). Large-scale experimental and theoretical study of graphene grain boundary structures. Phys. Rev. B, 92, 205402. https://doi.org/10.1103/PhysRevB.92.205402

  28. Kurasch, S., Kotakoski, J., Lehtinen, O., et al. (2012). Atom-by-Atom Observation of Grain Boundary Migration in Graphene. Nano Lett., 12, 3168–3173. https://doi.org/10.1021/nl301141g

  29. Yazyev, O.V. & Louie, S.G. (2010). Topological defects in graphene: Dislocations and grain boundaries. Phys. Rev. B, 81, 195420. https://doi.org/10.1103/PhysRevB.81.195420

  30. Egerton, R. (2019). Radiation damage to organic and inorganic specimens in the TEM. Micron, 119, 72–87. https://doi.org/10.1016/j.micron.2019.01.005

  31. Warner, J.H., Rümmeli, M.H., Bachmatiuk, A., et al. (2010). Examining the stability of folded graphene edges against electron beam induced sputtering with atomic resolution. Nanotechnology, 21, 325702. https://doi.org/10.1088/0957-4484/21/32/325702

  32. Warner, J.H., Rümmeli, M.H., Ge, L., et al. (2009). Structural transformations in graphene studied with high spatial and temporal resolution. Nat. Nanotechnol., 4, 500–504. https://doi.org/10.1038/nnano.2009.194

  33. Rummeli, M.H., Ta, H.Q., Mendes, R.G., et al. (2019). New Frontiers in Electron Beam–Driven Chemistry in and around Graphene. Adv. Mater., 31, 1800715. https://doi.org/10.1002/adma.201800715

  34. Egerton, R.F., Wang, F. & Crozier, P.A. (2006). Beam-Induced Damage to Thin Specimens in an Intense Electron Probe. Microsc. Microanal., 12, 65–71. https://doi.org/10.1017/S1431927606060065

  35. Li, L., Reich, S. & Robertson, J. (2005). Defect energies of graphite: Density-functional calculations. Phys. Rev. B, 72, 184109. https://doi.org/10.1103/PhysRevB.72.184109

  36. Crespi, V.H., Chopra, N.G., Cohen, M.L., et al. (1996). Anisotropic electron-beam damage and the collapse of carbon nanotubes. Phys. Rev. B, 54, 5927–5931. https://doi.org/10.1103/PhysRevB.54.5927

  37. Zan, R., Ramasse, Q.M., Bangert, U., et al. (2012). Graphene Reknits Its Holes. Nano Lett., 12, 3936–3940. https://doi.org/10.1021/nl300985q

  38. Trentino, A., Madsen, J., Mittelberger, A., et al. (2021). Atomic-Level Structural Engineering of Graphene on a Mesoscopic Scale. Nano Lett., 21, 5179–5185. https://doi.org/10.1021/acs.nanolett.1c01214

  39. Banhart, F. (2025). The Formation and Transformation of Low‐Dimensional Carbon Nanomaterials by Electron Irradiation. Small, 21, 2310462. https://doi.org/10.1002/smll.202310462

  40. Bauer, T., Schlüter, A.D. & Sakamoto, J. (2010). Towards 2D and 3D Coordination Polymers: Synthesis of Shape-Persistent Star Monomers with 2,2′:6′,2′′-Terpyridin-4′-yl Units at the Periphery. Synlett, 2010, 877–880. https://doi.org/10.1055/s-0029-1219541

  41. Liu, X., He, M., Calvani, D., et al. (2020). Power generation by reverse electrodialysis in a single-layer nanoporous membrane made from core–rim polycyclic aromatic hydrocarbons. Nat. Nanotechnol., 15, 307–312. https://doi.org/10.1038/s41565-020-0641-5

  42. van der Ham, A., Liu, X., Calvani, D., et al. (2022). Freestanding non-covalent thin films of the propeller-shaped polycyclic aromatic hydrocarbon decacyclene. Nat. Commun., 13, 1920. https://doi.org/10.1038/s41467-022-29429-8

  43. He, M., Ding, Y. & Liu, X. (2024). Nanoporous Amorphous Carbon Monolayer Derived from Fullerene Film. Adv. Sci., 11, 2308187. https://doi.org/10.1002/advs.202308187

  44. Madsen, J., Liu, P., Kling, J., et al. (2018). A Deep Learning Approach to Identify Local Structures in Atomic‐Resolution Transmission Electron Microscopy Images. Adv. Theory Simul., 1, 1800037. https://doi.org/10.1002/adts.201800037

  45. Leist, C., He, M., Liu, X., et al. (2022). Deep-Learning Pipeline for Statistical Quantification of Amorphous Two-Dimensional Materials. ACS Nano, 16, 20488–20496. https://doi.org/10.1021/acsnano.2c06807