Polyoxometalates in Nanotubes

August 26, 2019 – Researchers from Nottingham and Ulm have found that polyoxometalates, negatively charged metal-oxide clusters about 1 nm wide, enter carbon nanotubes by themselves from water: the tubes hand electrons to the clusters and then pull them inside. AC-HRTEM at 80 kV on an FEI Titan in Ulm, backed by image simulations, resolved the encapsulated clusters molecule by molecule, and TEM at 100 kV in Nottingham validated the filling over large areas. AC-HRTEM at 80 kV on a JEOL ARM200F in Stuttgart shows the same molecule alike, and earlier HRTEM at 300 and 120 kV from London, Oxford and AIST in Tsukuba saw tungsten clusters move and fuse in nanotubes as in Ulm. Protected by the tube, the clusters survive 1000 charging cycles and alkaline solution.

Charged molecules and the water-repellent inside of a carbon nanotube were thought not to mix. Researchers from the University of Nottingham and Ulm University have now shown the opposite: polyoxometalates, metal-oxide clusters about 1 nm wide that carry several negative charges, slip into single-walled carbon nanotubes all by themselves when the tubes are simply stirred in their aqueous solution. No further reagents are needed. Aberration-corrected high-resolution transmission electron microscopy (AC-HRTEM) at 80 kV in Ulm, on an FEI Titan 80-300 with a Cs corrector, imaged the encapsulated clusters molecule by molecule and resolved the tungsten atoms inside them (Fig. 1). Image simulations confirmed what the images show. TEM at 100 kV on a JEOL 2100 in Nottingham showed that virtually every nanotube was filled and that the clusters stay intact, even after 1000 charging cycles and in alkaline solution, and energy-dispersive X-ray (EDX) spectroscopy measured their composition. Two independent studies validate the images: in Stuttgart, the same {W12} molecule imaged on graphene by AC-HRTEM at 80 kV on a Cs-corrected JEOL ARM200F looks alike, and a team from London, Oxford and AIST in Tsukuba had seen another tungsten POM move and fuse inside nanotubes, by HRTEM at 300 kV and Cs-corrected HRTEM at 120 kV, as it does in Ulm.

Charge stores in a carbon sleeve
Polyoxometalates, POMs for short, are clusters of early transition metal oxides, for example of tungsten or molybdenum, with a precisely defined composition and structure[1]. They can take up and release several electrons at once, which makes them candidates for molecular memories and for the redox components of batteries[2]. Two problems stand in the way: fully oxidized POMs do not conduct electricity, and they are often chemically unstable, especially in alkaline media. Carbon nanotubes conduct well and offer a large surface, so earlier work attached POMs to their outside, for example through organic cations[3] or organic “antenna” groups[4]. But POMs bound to the surface are easily knocked off[5].

Putting the clusters inside the tubes would protect them. HRTEM had already shown individual tungsten POMs inside double-walled nanotubes, filled from ethanol solution[6]. Yet highly charged ions were expected to be repelled by the hydrophobic channel, a view supported by calculations[7], and so most work encapsulated neutral species such as salts[8], metal and non-metal nanostructures[9],[10] and organic molecules[11].

A filling that runs by itself
The team used two tungsten POMs, [PW12O40]3−, called {W12}, and [P2W18O62]6−, called {W18}, both about 1 nm wide, and nanotubes from an arc discharge with an average diameter of 1.4 nm[12]. When the opened tubes were added to the aqueous POM solution, the solution turned dark blue where it touched the tubes, the colour of reduced tungsten POMs. The nanotubes give electrons to the POMs, become positively charged themselves, and then pull the negative clusters into their channel. A similar electron transfer from nanotubes to guest clusters had stabilized metal iodide clusters inside nanotubes (see Inorganic Synthesis in Carbon Nanotubes)[13]. The POMs fit the channel so closely that they must shed their water shell on entry, which drives the filling further. How the samples were made is described in the box below.

▸ Recipe: POMs into nanotubes

Molecules seen one by one
AC-HRTEM shows the POMs as dark, regularly spaced clusters inside the nanotubes (Fig. 1). The clusters measure 1.0–1.8 nm across, because each POM sits in another orientation inside the channel, much as they do on graphene[14]. Within single molecules, the images resolve tungsten–tungsten distances between 250 and 300 pm. Electron microscope images of the same samples taken at two voltages and with two microscopes agree, as the box below shows with the overview images (Fig. 2) and two tables.

▸ Validation: FEI Titan at 80 kV vs. JEOL 2100 at 100 kV

What the composition tells
EDX spectra of the filled tubes show tungsten and oxygen but no significant potassium, although the POMs were used as potassium salts. The potassium ions stayed in the solution, so the positively charged nanotube itself balances the charge of the POM. The tungsten-to-oxygen ratios and the spacing of the clusters along the tubes are compared in the box below (Table 3).

▸ Comparison: TEM and EDX vs. the formulas

Watching the beam at work
At 80 kV, single molecules can be followed over time. A {W12} cluster turns and shifts inside its tube over 30 seconds (Fig. 3). The electron beam also changes the sample: in both materials it cut the nanotubes and fused several POMs into larger clusters (Fig. 4). This fragmentation and recombination explains part of the spread in cluster sizes. Exposure times were therefore kept as short as possible. A smaller tungsten POM, imaged by a team from London, Oxford and Tsukuba eleven years earlier, behaved the same way under the beam, as the box below shows (Tables 4 and 5).

▸ Validation: FEI Titan at 80 kV vs. JEOL 3000F at 300 kV and JEOL 2010F at 120 kV

Images and simulation agree
To confirm the structures, models of the POMs were placed inside nanotube models of the chirality seen in each image, and their images were simulated for the conditions of the experiment. The simulated images match the experimental ones for both POMs, as the box below shows (Fig. 5, Table 6).

▸ Validation: AC-HRTEM vs. image simulation

The same {W12} molecule had been imaged one by one at 80 kV in another laboratory in 2018, on graphene instead of inside a nanotube; the box below compares the two (Fig. 6).

▸ Validation: FEI Titan at 80 kV vs. JEOL ARM200F at 80 kV

Robust in acid and in base
The encapsulated POMs remain fully functional: they can still be charged and discharged through the nanotube walls. After 1000 charge–discharge cycles, {W18}@SWNT kept 58 % of its initial charge, while free {W18} lost all activity under the same conditions. TEM afterwards shows most POMs still intact inside the tubes. In sodium hydroxide at pH 13, where free POMs decompose at once, the clusters inside the tubes survived as well.

Challenges named by the authors
The electron beam used for imaging cuts the nanotubes and fuses POMs, so the sizes measured in the images partly reflect the imaging itself. The nanotubes must be freshly opened: oxygen adsorbed from air lowers their ability to give electrons and spoils the filling.

Outlook
Nanotubes and POMs assemble into a durable hybrid on their own, in water at room temperature. “The reagent-free redox-driven nanoconfinement of hydrophilic polyanionic materials within hydrophobic nanoscale carbon channels (which until now were considered incompatible) opens up new opportunities for the scalable and sustainable synthesis of hybrid functional materials,” the authors conclude. AC-HRTEM at 80 kV in Ulm made it possible to check the molecules inside the tubes one by one.

Resource:
Jordan, J. W., Lowe, G. A., McSweeney, R. L., Stoppiello, C. T., Lodge, R. W., Skowron, S. T., Biskupek, J., Rance, G. A., Kaiser, U., Walsh, D. A., Newton, G. N., Khlobystov, A. N. (2019).
Host–Guest Hybrid Redox Materials Self-Assembled from Polyoxometalates and Single-Walled Carbon Nanotubes.
Adv. Mater. 31(41), 1904182.
https://doi.org/10.1002/adma.201904182

Download this news article as PDF – for reading on paper, taking notes or filing.

References
  1. Long, D., Burkholder, E., Cronin, L. (2007). Polyoxometalate Clusters, Nanostructures and Materials: From Self Assembly to Designer Materials and Devices. Chem. Soc. Rev., 36, 105–121. https://doi.org/10.1039/B502666K

  2. Gumerova, N. I., Rompel, A. (2018). Synthesis, Structures and Applications of Electron-Rich Polyoxometalates. Nat. Rev. Chem., 2, 0112. https://doi.org/10.1038/s41570-018-0112

  3. Toma, F. M., Sartorel, A., Iurlo, M., Carraro, M., Parisse, P., Maccato, C., Rapino, S., Gonzalez, B. R., Amenitsch, H., Da Ros, T., Casalis, L., Goldoni, A., Marcaccio, M., Scorrano, G., Scoles, G., Paolucci, F., Prato, M., Bonchio, M. (2010). Efficient Water Oxidation at Carbon Nanotube–Polyoxometalate Electrocatalytic Interfaces. Nat. Chem., 2, 826–831. https://doi.org/10.1038/nchem.761

  4. Ma, D., Liang, L., Chen, W., Liu, H., Song, Y. (2013). Covalently Tethered Polyoxometalate–Pyrene Hybrids for Noncovalent Sidewall Functionalization of Single-Walled Carbon Nanotubes as High-Performance Anode Material. Adv Funct Materials, 23, 6100–6105. https://doi.org/10.1002/adfm.201301624

  5. Hu, J., Ji, Y., Chen, W., Streb, C., Song, Y. (2016). “Wiring” Redox-Active Polyoxometalates to Carbon Nanotubes Using a Sonication-Driven Periodic Functionalization Strategy. Energy Environ. Sci., 9, 1095–1101. https://doi.org/10.1039/C5EE03084F

  6. Sloan, J., Matthewman, G., Dyer-Smith, C., Sung, A., Liu, Z., Suenaga, K., Kirkland, A. I., Flahaut, E. (2008). Direct Imaging of the Structure, Relaxation, and Sterically Constrained Motion of Encapsulated Tungsten Polyoxometalate Lindqvist Ions Within Carbon Nanotubes. ACS Nano, 2, 966–976. https://doi.org/10.1021/nn7002508

  7. Medeiros, P. V. C., Marks, S., Wynn, J. M., Vasylenko, A., Ramasse, Q. M., Quigley, D., Sloan, J., Morris, A. J. (2017). Single-Atom Scale Structural Selectivity in Te Nanowires Encapsulated Inside Ultranarrow, Single-Walled Carbon Nanotubes. ACS Nano, 11, 6178–6185. https://doi.org/10.1021/acsnano.7b02225

  8. Meyer, R. R., Sloan, J., Dunin-Borkowski, R. E., Kirkland, A. I., Novotny, M. C., Bailey, S. R., Hutchison, J. L., Green, M. L. H. (2000). Discrete Atom Imaging of One-Dimensional Crystals Formed Within Single-Walled Carbon Nanotubes. Science, 289, 1324–1326. https://doi.org/10.1126/science.289.5483.1324

  9. Chamberlain, T. W., Zoberbier, T., Biskupek, J., Botos, A., Kaiser, U., Khlobystov, A. N. (2012). Formation of Uncapped Nanometre-Sized Metal Particles by Decomposition of Metal Carbonyls in Carbon Nanotubes. Chem. Sci., 3, 1919. https://doi.org/10.1039/c2sc01026g

  10. Zoberbier, T., Chamberlain, T. W., Biskupek, J., Kuganathan, N., Eyhusen, S., Bichoutskaia, E., Kaiser, U., Khlobystov, A. N. (2012). Interactions and Reactions of Transition Metal Clusters With the Interior of Single-Walled Carbon Nanotubes Imaged at the Atomic Scale. J. Am. Chem. Soc., 134, 3073–3079. https://doi.org/10.1021/ja208746z

  11. Skowron, S. T., Chamberlain, T. W., Biskupek, J., Kaiser, U., Besley, E., Khlobystov, A. N. (2017). Chemical Reactions of Molecules Promoted and Simultaneously Imaged by the Electron Beam in Transmission Electron Microscopy. Acc. Chem. Res., 50, 1797–1807. https://doi.org/10.1021/acs.accounts.7b00078

  12. Britz, D. A., Khlobystov, A. N. (2006). Noncovalent Interactions of Molecules With Single Walled Carbon Nanotubes. Chem. Soc. Rev., 35, 637. https://doi.org/10.1039/b507451g

  13. Botos, A., Biskupek, J., Chamberlain, T. W., Rance, G. A., Stoppiello, C. T., Sloan, J., Liu, Z., Suenaga, K., Kaiser, U., Khlobystov, A. N. (2016). Carbon Nanotubes as Electrically Active Nanoreactors for Multi-Step Inorganic Synthesis: Sequential Transformations of Molecules to Nanoclusters and Nanoclusters to Nanoribbons. J. Am. Chem. Soc., 138, 8175–8183. https://doi.org/10.1021/jacs.6b03633