Nanoprotrusions on Nanotubes

August 14, 2011 – Can the inside of a carbon nanotube take part in a chemical reaction? Single rhenium atoms, carried into single-walled nanotubes on a fullerene, make the inert inner wall reactive. AC-HRTEM at 80 kV on the image-side corrected FEI Titan in Ulm shows how a hollow bulge about 1 nm wide grows out of the sidewall in three stages, and calculations from Nottingham explain why rhenium can do this. An independent study from Oxford at 80 kV, with praseodymium instead, serves as validation.

The outer surface of a single-walled carbon nanotube is chemically reactive: its convex arrangement of carbon atoms is ideal for bonding to reagent molecules without damaging the tube[1]. For the same reason, the concave inner surface has been regarded as essentially inert. Nanotubes have therefore been used as reaction vessels for aggressive chemical processes, and in each case they acted purely as inert containers[2]. To use nanotubes as true nanoreactors, however, the reactivity of their inner surface has to be explored.

With aberration-corrected HRTEM at 80 kV on the FEI Titan in Ulm, Thomas Chamberlain and Andrei Khlobystov in Nottingham, together with Jannik Meyer, Johannes Biskupek, Jens Leschner and Ute Kaiser at Ulm University, have now shown that the inner wall can react after all[3]. The trigger is a single rhenium atom, carried into the nanotube on a fullerene. Under the electron beam, a hollow bulge about 1 nm wide grows out of the sidewall in three stages. Quantum chemical calculations and molecular dynamics simulations by the Nottingham team explain why rhenium makes the wall reactive. An independent study from Oxford, with praseodymium instead of rhenium and the JEOL JEM-2200MCO at 80 kV[4], serves as validation.

A test tube with a catalyst
Reactions of fullerenes inside nanotubes, triggered by the electron beam, had already been followed in the microscope[5]. The Ulm team deliberately lowered the energy of the electrons to 80 keV, below the threshold of 86 keV at which the beam knocks carbon atoms out of a nanotube[6]. A perfect nanotube therefore stays intact under these imaging conditions. The fullerene cages inside it are less robust: the beam damages them, and they merge into a corrugated inner tube without reacting with the wall of the outer one.

Transition metals catalyse a wide range of chemical reactions, including the breaking and formation of carbon–carbon bonds. Placing a transition metal inside a nanotube may therefore engage the interior in chemical reactions. The team chose rhenium because it has one of the widest ranges of oxidation states among the transition metals and catalyses several reactions involving carbon–carbon bonds[7]. To bring single rhenium atoms into the tube, a rhenium atom was bound to one of the pentagonal faces of C60, forming the complex Re(η5-C60H5)(CO)3[8] (Fig. 1a). The strong van der Waals attraction between the fullerene cage and the nanotube interior, up to 290 kJ/mol[9], pulled the complexes into the tubes at room temperature (Fig. 1b). About 20% of the nanotubes were filled.

In the images, the rhenium atoms appear as dark dots next to the fullerene cages (Fig. 1c). The complex proved much more sensitive to the beam than other fullerenes studied in nanotubes[10]. The cages were damaged almost at once, coalesced, and the rhenium atoms came loose as the pentagonal faces that bound them disappeared (Fig. 1d). Atoms that move faster than the exposure time of one second are smeared out and become invisible, so fewer rhenium atoms could be seen as the inner tube smoothed out. Energy-dispersive X-ray spectroscopy confirmed that the rhenium stayed inside the nanotube throughout the experiment (Fig. 1e).

Three stages of a bulge
Metal atoms in endohedral fullerenes behave similarly at first: once the beam damages the cage, they escape into the nanotube[11]. At 80 kV they move randomly within the tube or form small clusters[12], as described in the SALVE news article Reactions in a Nano-Container. The highly catalytic rhenium atoms, immersed in the carbon-rich debris of the decomposing fullerenes, behaved differently. Once the original complex had completely fragmented, the sidewall deformed slightly next to individual rhenium atoms. In some cases the deformed wall ruptured, and hollow protrusions about 1 nm in diameter developed rapidly (Fig. 2). The process was very fast at the start, which made the detailed mechanism hard to capture, and slowed down as the protrusion grew. Rhenium atoms were present only briefly in the reaction zone; in some image series a rhenium atom moved into and out of the protrusion repeatedly (Fig. 2b).

Every newly formed protrusion was dynamic and skewed. Over time under the beam, it annealed into a symmetric shape that stayed unchanged for long periods, so its structure could be imaged with atomic resolution. The images show closed structures of hexagons and other rings; the topology demands pentagons in the cap and heptagons at the base. In all, the images show three key stages: (i) the sidewall deforms and ruptures, (ii) an asymmetric, open protrusion forms quickly, and (iii) the protrusion slowly closes and becomes symmetric. These stages occurred in every protrusion observed, on nanotubes of different diameters and chiralities (Fig. 3).

Videos 1 and 2 show how a protrusion forms from inside the tube, and that the process speeds up at a higher beam intensity. To capture it from the beginning, the beam was first reduced to the absolute minimum, about 3 × 105 electrons/nm2 per frame, and then raised gradually to about 1 × 107 electrons/nm2 per frame. The first signs of a protrusion appeared after a total dose of about 2 × 106 electrons/nm2. The videos therefore start with a grainy, noisy screen. The atoms first appear white (overfocus) until the focus is adjusted and they turn black (underfocus). At the end, the symmetric protrusion can be seen clearly.

Video 1: A nanoprotrusion grows out of the sidewall of a single-walled nanotube filled with the rhenium–fullerene complex, AC-HRTEM at 80 kV. The beam starts at minimum intensity, so the first frames are noisy; the atoms appear white (overfocus) until the focus is adjusted (supplementary video of the paper).

Video 2: A second nanoprotrusion forming, from the noisy start at minimum beam intensity to the closed, symmetric protrusion at the end, AC-HRTEM at 80 kV (supplementary video of the paper).

Both ingredients are needed. Control experiments with fullerenes alone and with rhenium alone, compared in the box below (Fig. 4 and Fig. 5), left the wall without protrusions: rhenium acts as the catalyst, and the fullerenes supply the carbon.

▸ Comparison: rhenium–fullerene complex vs. C60 alone vs. rhenium alone

Why rhenium opens the wall
Fullerene cages exposed to radiation, including an electron beam, can lose or gain carbon in the form of C2 units[14], which are seen as the fundamental building blocks of carbon nanostructures[15]. According to density functional theory (DFT) calculations, a C2 unit alone does not react with the inner surface of a nanotube; it binds with less than 20 kJ/mol. This agrees with the control experiments with C60. Rhenium, however, has a high affinity for carbon[16], and C2 readily binds to it to form ReC2 (Fig. 6a).

The beam acts as an oxidant that removes valence electrons from rhenium. The calculations show strong binding to C2 for rhenium in the oxidation states I to III, the strongest for Re(III), while Re(IV) and higher states form no stable bond. In Re(III)C2, the highest occupied molecular orbital changes its shape and becomes localized almost entirely on the terminal carbon atom, ready for an end-on attack on the tube wall. The binding of ReC2 to the inner surface of the nanotube, relative to C2 alone, rises steeply with the oxidation state of rhenium, to more than a hundredfold for Re(III) (Fig. 6b). The bond is not just covalent: a large amount of charge flows from the sidewall to the metal.

The bonded ReC2 stretches the carbon–carbon bonds of the sidewall nearby by up to 6% (Fig. 6c). This weakens them and lowers the knock-on threshold locally, creating a weak point that the beam can damage even at 80 kV. The resulting vacancy with dangling bonds becomes the nucleus of a protrusion (Fig. 6d). In most experiments, no defects were seen on the nanotube before stage 1, so rhenium can catalyse reactions with the structurally perfect inner surface. Molecular dynamics simulations show that further C2 units attach spontaneously to the open edge of the growing protrusion, without help from rhenium. This explains the fast stage 2 and why rhenium stays only briefly in the reaction zone.

An unlimited supply of carbon could in principle let the protrusion grow into a long tentacle. Instead, its growth is limited by curvature: pentagons form at the edge, which curls and so reduces the number of dangling bonds, similar to the mechanism by which fullerenes form from graphene[17] (SALVE news article Fullerenes from Graphene). Asymmetric protrusions still carry some dangling bonds, so they keep changing shape under the beam, as seen in stage 2. The most stable form is a sealed protrusion with no dangling bonds and the strain evenly distributed (Fig. 6e), as seen in stage 3; once formed, it no longer changes its size or shape under the beam. Its last dangling bonds disappear, and with them any site where rhenium could bind, so the metal does not become part of the final structure.

An independent study from Oxford followed another metal in nanotubes at the same voltage. The box below sets both studies side by side, with the Oxford images of a metal atom leaving its cage (Fig. 7), clusters merging into a crystal (Fig. 8) and the image simulations of that crystal (Fig. 9).

▸ Validation: FEI Titan at 80 kV (Ulm) vs. JEOL JEM-2200MCO at 80 kV (Oxford)

Buds from the inside
The protrusions are topologically similar to nanobuds, fullerene-like bulges on nanotubes that were discovered in Helsinki[18]. Materials with such negatively curved surfaces attract interest because of their electronic properties[19]. Nanobuds, however, form from fullerene molecules adsorbed on the outer surface and fused with it. The Ulm images show that protrusions can grow from the inside of the nanotube, provided that a transition-metal catalyst sits in its cavity.

▸ Recipe: sample, microscope and calculations

Challenges named by the authors
The elementary steps of the reaction are much faster than the capture rate of one image per second, so the images show snapshots of the three stages but not the precise mechanism. Rhenium atoms that move faster than the exposure time become invisible, and only spectroscopy proves that they are still in the tube. The fate of the carbonyl groups and hydrogen atoms could not be followed; they are assumed to leave the tube into the vacuum of the microscope. The first stages are so fast that the beam had to start at the lowest dose that still allowed the region to be found, so the start of each series is noisy and not exactly in focus. Defects already present in the sidewall may take part in some cases. The calculations show that the chemistry of rhenium suits this reaction; other transition metals do not necessarily behave the same way.

A reactive inside
The inner surface of a nanotube, even more inert than graphene, can be engaged in chemical reactions by transition-metal atoms, and low-voltage aberration-corrected HRTEM can follow these reactions atom by atom. "This may open new avenues for catalytic applications of this metal to produce new types of carbon nanostructures with exciting functional properties," the authors write.

At 80 kV the beam still damages the fullerenes and drives the reaction. With low-voltage electron microscopy, the SALVE project set out to reduce such beam damage further, so that molecules and their reactions can be watched for longer; its work continues today in the SALVE Microscopy Center in Ulm.

Resource:
Chamberlain, T. W., Meyer, J. C., Biskupek, J., Leschner, J., Santana, A., Besley, N. A., Bichoutskaia, E., Kaiser, U., Khlobystov, A. N. (2011).
Reactions of the inner surface of carbon nanotubes and nanoprotrusion processes imaged at the atomic scale.
Nature Chem. 3(9), 732–737.
https://doi.org/10.1038/nchem.1115

Download this news article as PDF – for reading on paper, taking notes or filing.

References
  1. Tasis, D., Tagmatarchis, N., Bianco, A., & Prato, M. (2006). Chemistry of Carbon Nanotubes. Chemical Reviews, 106, 1105–1136. https://doi.org/10.1021/cr050569o

  2. Britz, D. A., Khlobystov, A. N., Porfyrakis, K., Ardavan, A., & Briggs, G. A. D. (2005). Chemical Reactions Inside Single-Walled Carbon Nano Test-Tubes. Chemical Communications, 37. https://doi.org/10.1039/b414247k

  3. Chamberlain, T. W., Meyer, J. C., Biskupek, J., Leschner, J., Santana, A., Besley, N. A., Bichoutskaia, E., Kaiser, U., & Khlobystov, A. N. (2011). Reactions of the Inner Surface of Carbon Nanotubes and Nanoprotrusion Processes Imaged at the Atomic Scale. Nature Chemistry, 3(9), 732–737. https://doi.org/10.1038/nchem.1115

  4. Warner, J. H., Plant, S. R., Young, N. P., Porfyrakis, K., Kirkland, A. I., & Briggs, G. A. D. (2011). Atomic Scale Growth Dynamics of Nanocrystals Within Carbon Nanotubes. ACS Nano, 5(2), 1410–1417. https://doi.org/10.1021/nn1031802

  5. Koshino, M., Niimi, Y., Nakamura, E., Kataura, H., Okazaki, T., Suenaga, K., & Iijima, S. (2010). Analysis of the Reactivity and Selectivity of Fullerene Dimerization Reactions at the Atomic Level. Nature Chemistry, 2, 117–124. https://doi.org/10.1038/nchem.482

  6. Egerton, R. F., Li, P., & Malac, M. (2004). Radiation Damage in the TEM and SEM. Micron, 35, 399–409. https://doi.org/10.1016/j.micron.2004.02.003

  7. Grubbs, R. H. (1982). Alkene and Alkyne Metathesis Reactions. In G. Wilkinson, F. G. A. Stone, & E. W. Abel (Eds.), Comprehensive Organometallic Chemistry, Vol. 8, Ch. 54. Pergamon.

  8. Toganoh, M., Matsuo, Y., & Nakamura, E. (2003). Rhenium‐Templated Regioselective Polyhydrogenation Reaction of [60]Fullerene. Angewandte Chemie International Edition, 42, 3530–3532. https://doi.org/10.1002/anie.200351722

  9. Ulbricht, H., Moos, G., & Hertel, T. (2003). Interaction of C60 With Carbon Nanotubes and Graphite. Physical Review Letters, 90(9), 095501. https://doi.org/10.1103/PhysRevLett.90.095501

  10. Suenaga, K., Okazaki, T., Wang, C.-R., Bandow, S., Shinohara, H., & Iijima, S. (2003). Direct Imaging of Sc2@C84 Molecules Encapsulated Inside Single-Wall Carbon Nanotubes by High Resolution Electron Microscopy With Atomic Sensitivity. Physical Review Letters, 90(5), 055506. https://doi.org/10.1103/PhysRevLett.90.055506

  11. Jin, C., Lan, H., Suenaga, K., Peng, L., & Iijima, S. (2008). Metal Atom Catalyzed Enlargement of Fullerenes. Physical Review Letters, 101, 176102. https://doi.org/10.1103/PhysRevLett.101.176102

  12. Chuvilin, A., Khlobystov, A. N., Obergfell, D., Haluska, M., Yang, S., Roth, S., & Kaiser, U. (2009). Observations of Chemical Reactions at the Atomic Scale: Dynamics of Metal‐Mediated Fullerene Coalescence and Nanotube Rupture. Angewandte Chemie International Edition, 49, 193–196. https://doi.org/10.1002/anie.200902243

  13. Hernández, E., Meunier, V., Smith, B. W., Rurali, R., Terrones, H., Nardelli, M. B., Terrones, M., Luzzi, D. E., & Charlier, J. C. (2003). Fullerene Coalescence in Nanopeapods: A Path to Novel Tubular Carbon. Nano Letters, 3, 1037–1042. https://doi.org/10.1021/nl034283f

  14. Huang, J. Y., Ding, F., Jiao, K., & Yakobson, B. I. (2007). Real Time Microscopy, Kinetics, and Mechanism of Giant Fullerene Evaporation. Physical Review Letters, 99, 175503. https://doi.org/10.1103/PhysRevLett.99.175503

  15. Irle, S., Zheng, G., Wang, Z., & Morokuma, K. (2006). The C60 Formation Puzzle ‘Solved’: QM/MD Simulations Reveal the Shrinking Hot Giant Road of the Dynamic Fullerene Self-Assembly Mechanism. The Journal of Physical Chemistry B, 110, 14531–14545. https://doi.org/10.1021/jp061173z

  16. Chabanas, M., Baudouin, A., Copéret, C., & Basset, J.-M. (2001). A Highly Active Well-Defined Rhenium Heterogeneous Catalyst for Olefin Metathesis Prepared via Surface Organometallic Chemistry. Journal of the American Chemical Society, 123, 2062–2063. https://doi.org/10.1021/ja000900f

  17. Chuvilin, A., Kaiser, U., Bichoutskaia, E., Besley, N. A., & Khlobystov, A. N. (2010). Direct Transformation of Graphene to Fullerene. Nature Chemistry, 2, 450–453. https://doi.org/10.1038/nchem.644

  18. Nasibulin, A. G., Pikhitsa, P. V., Jiang, H., Brown, D. P., Krasheninnikov, A. V., Anisimov, A. S., Queipo, P., Moisala, A., Gonzalez, D., Lientschnig, G., Hassanien, A., Shandakov, S. D., Lolli, G., Resasco, D. E., Choi, M., Tománek, D., & Kauppinen, E. I. (2007). A Novel Hybrid Carbon Material. Nature Nanotechnology, 2, 156–161. https://doi.org/10.1038/nnano.2007.37

  19. He, H. Y., & Pan, B. C. (2009). Electronic Structures and Raman Features of a Carbon Nanobud. The Journal of Physical Chemistry C, 113, 20822–20826. https://doi.org/10.1021/jp906026c

  20. Shao, Y., Molnar, L. F., Jung, Y., Kussmann, J., Ochsenfeld, C., Brown, S. T., Gilbert, A. T. B., Slipchenko, L. V., Levchenko, S. V., O’Neill, D. P., Jr, R. A. D., Lochan, R. C., Wang, T., Beran, G. J. O., Besley, N. A., Herbert, J. M., Lin, C. Y., Voorhis, T. V., Chien, S. H., … Head-Gordon, M. (2006). Advances in Methods and Algorithms in a Modern Quantum Chemistry Program Package. Phys. Chem. Chem. Phys., 8, 3172–3191. https://doi.org/10.1039/B517914A

  21. Brenner, D. W. (1990). Empirical Potential for Hydrocarbons for Use in Simulating the Chemical Vapor Deposition of Diamond Films. Physical Review B, 42, 9458–9471. https://doi.org/10.1103/PhysRevB.42.9458

  22. Gale, J. D., & Rohl, A. L. (2003). The General Utility Lattice Program (GULP). Molecular Simulation, 29, 291–341. https://doi.org/10.1080/0892702031000104887