November 1, 2021 – Salt crystals only a few atomic layers thick survive in the electron microscope only as long as their graphene wrapper is intact. Researchers from Ulm, Dresden and Aalto imaged quasi-two-dimensional NaCl crystals sealed between two graphene sheets with Cs-corrected HRTEM at 80 kV and watched them decompose within seconds once a single hole appeared in the graphene. DFT calculations showed that free-standing crystals would disintegrate quickly, and larger crystals proved to be destroyed sooner than small ones, so only high-quality graphene can protect ionic crystals from beam damage.
Table salt is about the last thing one would expect to be fragile. Yet a crystal of sodium chloride (NaCl) only a few atomic layers thick does not survive long in a transmission electron microscope (TEM): the electron beam that images it also takes it apart. Scientists from Ulm University, the Helmholtz-Zentrum Dresden-Rossendorf and Aalto University in Finland have now watched such quasi-two-dimensional salt crystals, sealed between two sheets of graphene, as they decomposed under an 80 kV electron beam. With aberration-corrected high-resolution TEM (HRTEM) and density-functional theory (DFT) calculations, they showed that the graphene shields the salt only as long as the graphene itself is intact. As soon as a single hole appears, the crystal disintegrates within seconds, and, counterintuitively, larger crystals are destroyed faster than small ones.
Graphene as a protective wrapper
Graphene is a popular support material for high-resolution TEM[1]. It is mechanically strong, conducts electricity and heat very well[2]–[4], is only one atom thick, is chemically inert[5] and withstands electron irradiation up to energies of 80 keV[6]. Materials can also be sealed between two graphene sheets, which makes in situ studies of radiation- and environment-sensitive systems possible[7]–[10]. Not only solids, such as two-dimensional (2D) transition metal dichalcogenides[11]–[14], but also liquids can be encapsulated this way. The solid systems with their sandwich geometry are called vertical heterostructures[14], the liquid ones graphene liquid cells (GLCs)[15],[16].
How the beam does damage
What happens to the encapsulated material is often decided by the electron beam itself[17],[18]. Its interactions with a specimen fall into two main categories[19]. In the first, an energetic electron transfers momentum to an atomic nucleus and knocks the atom out of its place, the so-called knock-on damage. In the second, the electron interacts with the electrons of the specimen and excites the valence electrons (radiolysis) or removes them altogether (ionization)[19]–[21].
Defects can also arise through chemical etching, caused by reactive species left on the sample surface after preparation or present in the microscope column[22]. The electron beam can speed this up: residues such as oxygen molecules are split by ionization into radicals, which then attack the sample surface[23]. Below 80 keV, chemical etching is very likely the main damage mechanism in graphene[24], and metal- and vapor-mediated etching starts mainly at defects or contaminated areas, not in the pristine lattice[25].
How stable materials between graphene sheets are, and by which mechanisms they are damaged, was not fully understood. Ionic crystals such as NaCl are particularly sensitive to radiation[26],[27], which should produce chlorine radicals and promote the etching of graphene. It is therefore surprising that graphene enclosures are stable at all and that the ionic crystals inside can be imaged by TEM[28],[29], even though they are eventually destroyed. The team set out to understand, at the microscopic level, what decides how long the system survives under the beam.
Salt crystals that wait, then vanish
The researchers placed a drop of dilute salt solution between two graphene-covered TEM grids. As the water evaporated, cubic, quasi-2D NaCl crystals formed between the sheets by supersaturation, just like NaCl crystals observed earlier between graphene layers[30]. Comparisons with image simulations showed that the crystals were about four to eight atomic layers thick. How the samples were made and imaged is described in the box below.
In all experiments, the crystals at first did not change their projected size at all: the encapsulated NaCl did not start to disintegrate right away. The typical crystal in Fig. 1 had a projected area of about 220 nm2 and was imaged at a dose rate of about 6.1 × 105 electrons per nm2 and second. Fig. 1a shows the raw HRTEM images; in Fig. 1b the two graphene layers are coloured red and blue and the NaCl crystal green, the same colours as in the Fourier transform (FFT). The crystal remained stable for 533 s under the beam, then it began to decompose, and at the same moment a hole appeared in one of the two protecting graphene layers. Because graphene has little contrast next to the salt, such defects are hard to pick out with optical filtering, but they can be identified by eye.
A hole in the graphene starts the end
In every experiment, the NaCl crystals began to decompose around a hole in the graphene: the salt is stable only as long as its wrapper is undamaged. Even a single point defect is probably enough to start the process, because damaged graphene is more vulnerable to further degradation[32], and the hole grows through chemical etching by the chlorine radicals that the beam produces in the salt. The same happened with a much larger crystal of 2500 nm2 (Fig. 2), which first grew for about 133 s and then decomposed, again starting where the graphene was damaged. Further examples of such holes are shown in the box below (Fig. 3).
Graphene itself is highly resistant to ionization, radiolysis and knock-on damage up to electron energies of about 85 keV, so the defects in it are most likely produced by chemical etching[24], again probably by the chlorine radicals created in the salt. Once a first defect exists in the pristine lattice, it can grow, because atoms at its edge are easier to displace and knock-on damage becomes possible[32],[33]; defects also speed up the etching itself[25],[34]. As soon as the first defect appears in the graphene, the NaCl flake decomposes quickly.
Why free salt would not survive
To understand the decomposition, the team calculated with DFT how much energy is needed to knock sodium and chlorine atoms out of a NaCl flake, from its flat (100) surface and from its edges. As in earlier work[6],[35], the recoil atom was given an initial kinetic energy and its path was followed by molecular dynamics. The thinnest possible crystal, two atomic planes thick, was used; it is metastable even without support, because the (100) surface energy of NaCl is extremely low, about 10 meV per Å2[36]. Electronic excitations and charge build-up can affect a material under the beam[37], but they were left out, as the conducting graphene sheets around the crystal should mitigate them. Because the displaced ions are charged, the calculated thresholds had to be corrected for Coulomb interactions, as explained in the box below (Figs. 4 and 5).
So the graphene does more than wrap the salt. It stops the displaced atoms, which can then immediately recombine with the crystal. Ionic crystals are also damaged by ionization and radiolysis[26], but as long as the displaced Na+ and Cl− ions stay inside the enclosure, they return to the crystal, either to their former site or to another empty one. This leaves small rectangular defects that wander through the NaCl lattice, as a video of the experiment shows. They do not change how fast the crystal as a whole grows or decays, but they reveal how mobile the ions are inside the graphene pocket. Once a hole appears, the ions can escape and no longer recombine; they also etch the edges of the hole, which keeps growing, as the white frames in Fig. 1b show.
Bigger crystals die sooner
The team measured the projected area of ten NaCl crystals against the accumulated electron dose until each had disappeared (Fig. 6). All curves show the same pattern: a long stable phase, followed by a sudden collapse. To put numbers on it, the researchers fitted a logistic decay function to each curve. Its turning point marks the critical dose at which half of the crystal is gone and also the moment of the fastest decay; its slope gives the decay rate per electron. For the 220 nm2 crystal, the fit describes the data well up to a total dose of about 4.5 × 108 electrons per nm2 (Fig. 7, inset). The crystal of 320 nm2 decayed fastest; it began to decompose at two places at once, which suggests that its graphene was damaged at two points. Apart from this case, the number of holes in the graphene showed no clear link to the decay rate.
Plotting crystal size against critical dose revealed a striking trend (Fig. 7): the three largest crystals, of 1200, 1215 and 2500 nm2, survived only a very short exposure, much shorter than the typical crystals of 220 nm2 or less. The researchers explain this with a probability per area for the first defect to appear in graphene. The larger the graphene area over the crystal, the more likely it is that the beam creates a point defect somewhere, and that single defect is enough to start the decomposition of the whole crystal.
What it opens up
The study provides quantitative data on how long graphene-encapsulated quasi-2D salt crystals survive in the electron microscope, and it carries a clear message for anyone who wants to image sensitive materials in a graphene pocket: the wrapper must be flawless. “Our results provide quantitative data on the stability of encapsulated quasi 2D NaCl crystals and indicate that only high-quality graphene is suitable for protecting ionic crystals from beam damage in electron microscopy studies,” the authors conclude.
The insights reach beyond salt. According to the authors, they should help to protect other quasi-2D inorganic solids as well as liquids and organic molecules between graphene sheets, making future in situ electron microscopy experiments on such systems possible. The images behind these conclusions were recorded with aberration-corrected HRTEM at Ulm University and are also part of the dissertation of first author Tibor Lehnert[31].
Resource:
Lehnert, T., Kretschmer, S., Bräuer, F., Krasheninnikov, A. V., Kaiser, U. (2021).
Quasi-two-dimensional NaCl crystals encapsulated between graphene sheets and their decomposition under an electron beam.
Nanoscale 13(46), 19626–19633.
https://doi.org/10.1039/d1nr04792b
Download this news article as PDF – for reading on paper, taking notes or filing.
-
Sinha, S., Warner, J. H. (2021). Recent Progress in Using Graphene as an Ultrathin Transparent Support for Transmission Electron Microscopy. Small Structures, 2, 2000049. https://doi.org/10.1002/sstr.202000049
-
Ghosh, S., Calizo, I., Teweldebrhan, D., Pokatilov, E. P., Nika, D. L., Balandin, A. A., Bao, W., Miao, F., Lau, C. N. (2008). Extremely High Thermal Conductivity of Graphene: Prospects for Thermal Management Applications in Nanoelectronic Circuits. Applied Physics Letters, 92, 151911. https://doi.org/10.1063/1.2907977
-
Castro Neto, A. H., Guinea, F., Peres, N. M. R., Novoselov, K. S., Geim, A. K. (2009). The Electronic Properties of Graphene. Rev. Mod. Phys., 81, 109–162. https://doi.org/10.1103/RevModPhys.81.109
-
Balandin, A. A., Ghosh, S., Bao, W., Calizo, I., Teweldebrhan, D., Miao, F., Lau, C. N. (2008). Superior Thermal Conductivity of Single-Layer Graphene. Nano Lett., 8, 902–907. https://doi.org/10.1021/nl0731872
-
Zhang, Y., Zhang, L., Zhou, C. (2013). Review of Chemical Vapor Deposition of Graphene and Related Applications. Acc. Chem. Res., 46, 2329–2339. https://doi.org/10.1021/ar300203n
-
Meyer, J. C., Eder, F., Kurasch, S., Skakalova, V., Kotakoski, J., Park, H. J., Roth, S., Chuvilin, A., Eyhusen, S., Benner, G., et al. (2012). Accurate Measurement of Electron Beam Induced Displacement Cross Sections for Single-Layer Graphene. Phys. Rev. Lett., 108, 196102. https://doi.org/10.1103/PhysRevLett.108.196102
-
Kühne, M., Börrnert, F., Fecher, S., Ghorbani-Asl, M., Biskupek, J., Samuelis, D., Krasheninnikov, A. V., Kaiser, U., Smet, J. H. (2018). Reversible Superdense Ordering of Lithium Between Two Graphene Sheets. Nature, 564, 234–239. https://doi.org/10.1038/s41586-018-0754-2
-
Lin, Y., Motoyama, A., Kretschmer, S., Ghaderzadeh, S., Ghorbani-Asl, M., Araki, Y., Krasheninnikov, A. V., Ago, H., Suenaga, K. (2021). Polymorphic Phases of Metal Chlorides in the Confined 2D Space of Bilayer Graphene. Advanced Materials, 33, 2105898. https://doi.org/10.1002/adma.202105898
-
De Clercq, A., Dachraoui, W., Margeat, O., Pelzer, K., Henry, C. R., Giorgio, S. (2014). Growth of Pt–Pd Nanoparticles Studied In Situ by HRTEM in a Liquid Cell. J. Phys. Chem. Lett., 5, 2126–2130. https://doi.org/10.1021/jz500690a
-
Algara-Siller, G., Lehtinen, O., Wang, F. C., Nair, R. R., Kaiser, U., Wu, H. A., Geim, A. K., Grigorieva, I. V. (2015). Square Ice in Graphene Nanocapillaries. Nature, 519, 443–445. https://doi.org/10.1038/nature14295
-
Elibol, K., Susi, T., Argentero, G., Reza Ahmadpour Monazam, M., Pennycook, T. J., Meyer, J. C., Kotakoski, J. (2018). Atomic Structure of Intrinsic and Electron-Irradiation-Induced Defects in MoTe2. Chemistry of Materials, 30, 1230–1238. https://doi.org/10.1021/acs.chemmater.7b03760
-
Zan, R., Ramasse, Q. M., Jalil, R., Georgiou, T., Bangert, U., Novoselov, K. S. (2013). Control of Radiation Damage in MoS2 by Graphene Encapsulation. ACS Nano, 7, 10167–10174. https://doi.org/10.1021/nn4044035
-
Lehnert, T., Lehtinen, O., Algara–Siller, G., Kaiser, U. (2017). Electron Radiation Damage Mechanisms in 2D MoSe2. Applied Physics Letters, 110, 033106. https://doi.org/10.1063/1.4973809
-
Algara-Siller, G., Kurasch, S., Sedighi, M., Lehtinen, O., Kaiser, U. (2013). The Pristine Atomic Structure of MoS2 Monolayer Protected From Electron Radiation Damage by Graphene. Applied Physics Letters, 103, 203107. https://doi.org/10.1063/1.4830036
-
Textor, M., de Jonge, N. (2018). Strategies for Preparing Graphene Liquid Cells for Transmission Electron Microscopy. Nano Lett., 18, 3313–3321. https://doi.org/10.1021/acs.nanolett.8b01366
-
de Jonge, N., Houben, L., Dunin-Borkowski, R. E., Ross, F. M. (2018). Resolution and Aberration Correction in Liquid Cell Transmission Electron Microscopy. Nat Rev Mater, 4, 61–78. https://doi.org/10.1038/s41578-018-0071-2
-
Chamberlain, T. W., Biskupek, J., Skowron, S. T., Markevich, A. V., Kurasch, S., Reimer, O., Walker, K. E., Rance, G. A., Feng, X., Müllen, K., et al. (2017). Stop-Frame Filming and Discovery of Reactions at the Single-Molecule Level by Transmission Electron Microscopy. ACS Nano, 11, 2509–2520. https://doi.org/10.1021/acsnano.6b08228
-
Shin, D., Park, J. B., Kim, Y. J., Kim, S. J., Kang, J. H., Lee, B., Cho, S. P., Hong, B. H., Novoselov, K. S. (2015). Growth Dynamics and Gas Transport Mechanism of Nanobubbles in Graphene Liquid Cells. Nat Commun, 6, 6068. https://doi.org/10.1038/ncomms7068
-
Egerton, R., Li, P., Malac, M. (2004). Radiation Damage in the TEM and SEM. Micron, 35, 399–409. https://doi.org/10.1016/j.micron.2004.02.003
-
Zobelli, A., Gloter, A., Ewels, C. P., Seifert, G., Colliex, C. (2007). Electron Knock-on Cross Section of Carbon and Boron Nitride Nanotubes. Phys. Rev. B, 75, 245402. https://doi.org/10.1103/PhysRevB.75.245402
-
Banhart, F. (1999). Irradiation Effects in Carbon Nanostructures. Rep. Prog. Phys., 62, 1181–1221. https://doi.org/10.1088/0034-4885/62/8/201
-
Reimer, L., and Kohl, H. (2008). Transmission Electron Microscopy: Physics of Image Formation. Springer Series in Optical Sciences, 36, Springer, New York.
-
Talmon, Y. (1987). Electron Beam Radiation Damage to Organic and Biological Cryospecimens. Cryotechniques in Biological Electron Microscopy, 64–84. https://doi.org/10.1007/978-3-642-72815-0_3
-
Thiele, C., Felten, A., Echtermeyer, T. J., Ferrari, A. C., Casiraghi, C., v. Löhneysen, H., Krupke, R. (2013). Electron-Beam-Induced Direct Etching of Graphene. Carbon, 64, 84–91. https://doi.org/10.1016/j.carbon.2013.07.038
-
Ramasse, Q. M., Zan, R., Bangert, U., Boukhvalov, D. W., Son, Y. W., Novoselov, K. S. (2012). Direct Experimental Evidence of Metal-Mediated Etching of Suspended Graphene. ACS Nano, 6, 4063–4071. https://doi.org/10.1021/nn300452y
-
Hobbs, L. W. (1979). Radiation Effects in Analysis of Inorganic Specimens by TEM. Introduction to Analytical Electron Microscopy, 437–480. https://doi.org/10.1007/978-1-4757-5581-7_17
-
Egerton, R. (2021). Radiation Damage and Nanofabrication in TEM and STEM. Micros. Today, 29, 56–59. https://doi.org/10.1017/S1551929521000663
-
Vasu, K. S., Prestat, E., Abraham, J., Dix, J., Kashtiban, R. J., Beheshtian, J., Sloan, J., Carbone, P., Neek-Amal, M., Haigh, S. J., et al. (2016). Van der Waals pressure and its effect on trapped interlayer molecules. Nat Commun, 7, 12168. https://doi.org/10.1038/ncomms12168
-
Lehnert, T., Kinyanjui, M. K., Ladenburger, A., Rommel, D., Wörle, K., Börrnert, F., Leopold, K., Kaiser, U. (2017). In Situ Crystallization of the Insoluble Anhydrite AII Phase in Graphene Pockets. ACS Nano, 11, 7967–7973. https://doi.org/10.1021/acsnano.7b02513
-
Zhou, W., Yin, K., Wang, C., Zhang, Y., Xu, T., Borisevich, A., Sun, L., Idrobo, J. C., Chisholm, M. F., Pantelides, S. T., et al. (2015). The Observation of Square Ice in Graphene Questioned. Nature, 528, E1–E2. https://doi.org/10.1038/nature16145
-
Lehnert, T. (2020). Electron-Beam-Induced Modifications in Two-Dimensional Materials. PhD thesis, Ulm University.
-
Girit, C. O., Meyer, J. C., Erni, R., Rossell, M. D., Kisielowski, C., Yang, L., Park, C. H., Crommie, M. F., Cohen, M. L., Louie, S. G., et al. (2009). Graphene at the Edge: Stability and Dynamics. Science, 323, 1705–1708. https://doi.org/10.1126/science.1166999
-
Susi, T., Kotakoski, J., Arenal, R., Kurasch, S., Jiang, H., Skakalova, V., Stephan, O., Krasheninnikov, A. V., Kauppinen, E. I., Kaiser, U., et al. (2012). Atomistic Description of Electron Beam Damage in Nitrogen-Doped Graphene and Single-Walled Carbon Nanotubes. ACS Nano, 6, 8837–8846. https://doi.org/10.1021/nn303944f
-
Leuthner, G. T., Hummel, S., Mangler, C., Pennycook, T. J., Susi, T., Meyer, J. C., Kotakoski, J. (2019). Scanning Transmission Electron Microscopy Under Controlled Low-Pressure Atmospheres. Ultramicroscopy, 203, 76–81. https://doi.org/10.1016/j.ultramic.2019.02.002
-
Komsa, H. P., Kotakoski, J., Kurasch, S., Lehtinen, O., Kaiser, U., Krasheninnikov, A. V. (2012). Two-Dimensional Transition Metal Dichalcogenides Under Electron Irradiation: Defect Production and Doping. Phys. Rev. Lett., 109, 035503. https://doi.org/10.1103/PhysRevLett.109.035503
-
Kvashnin, A. G., Kvashnin, D. G., Oganov, A. R. (2019). Novel Unexpected Reconstructions of (100) and (111) Surfaces of NaCl: Theoretical Prediction. Sci Rep, 9, 14267. https://doi.org/10.1038/s41598-019-50548-8
-
Kretschmer, S., Lehnert, T., Kaiser, U., Krasheninnikov, A. V. (2020). Formation of Defects in Two-Dimensional MoS2 in the Transmission Electron Microscope at Electron Energies Below the Knock-on Threshold: The Role of Electronic Excitations. Nano Lett., 20, 2865–2870. https://doi.org/10.1021/acs.nanolett.0c00670