January 29, 2020 – In a large review on the production and processing of graphene and related materials, Ute Kaiser of Ulm University explains why these atom-thin materials must be imaged at 80 kV and less, and how the chromatic and spherical aberration corrector of the SALVE microscope keeps atomic resolution there: below one ångström from 40 to 80 kV and better than 0.14 nm even at 20 kV. Single-shot images of graphene at 80 kV show the gain over spherical aberration correction alone. At 80 kV, SALVE goes beyond the chromatic aberration corrected FEI Titan PICO in Jülich, and the design value of the chromatic and spherical aberration corrected TEAM I microscope.

Graphene and its two-dimensional relatives are only one atom or a few atoms thick, and every atom counts. High-resolution transmission electron microscopy (HRTEM) with aberration correction is the method of choice to see them, yet the fast electrons that form the image can also change what they image. In a large review by more than 130 authors, first author Claudia Backes, on the production and processing of graphene and related materials, Ute Kaiser of Ulm University wrote the section on low-energy HRTEM: why the acceleration voltage must come down for these materials, why that used to cost the atomic resolution, and how the chromatic aberration corrector of the SALVE microscope wins it back.

A beam that images and alters
For very thin samples such as single-layer graphene, the interaction of energetic electrons with the material may change its structure for good. This radiation damage is an obstacle for imaging, but also a tool for manipulating matter on the atomic scale: the beam can turn graphene into a two-dimensional amorphous carbon[1] or, atom by atom, into a 2D carbon glass[2], as shown at 80 to 100 kV in Ulm. These stories are told in the news articles From Graphene to 2D Amorphous Carbon and Carbon Glass.

The best investigated mechanism is knock-on damage, in which the fast electrons gradually push atoms out of the sample[3]. From the kinematics of the collision it follows that the damage can be prevented if the energy transferred stays below a certain threshold[4]. Depending on the material, this calls for acceleration voltages of 80 kV and less[5].

Low voltage used to mean low resolution
At such voltages a conventional TEM without aberration correction cannot resolve atoms: already at 80 kV its resolution is worse than 0.35 nm. High-end microscopes are therefore equipped with a corrector for the spherical aberration (Cs) and usually operate between 300 and 80 kV. They reach about 0.8 Å at 300 kV and about 1.9 Å at 80 kV, enough to resolve single atomic columns in many bulk crystals. Pristine single-layer graphene withstands 80 kV long enough for HRTEM images with a good signal-to-noise ratio, but edges and pores change much faster and need much lower voltages[5].

Below 80 kV, however, the resolving power of Cs-corrected microscopes is no longer sufficient, because the chromatic aberration Cc of the objective lens limits it: electrons of slightly different energy are focused at different heights. Two approaches tackle this limit. One reduces the energy width of the beam, with a cold field-emission gun or a monochromator[6],[7]. The other, and the most efficient one, corrects the chromatic aberration itself[8].

SALVE: sub-ångström from 40 to 80 kV
The Sub-Ångström Low-Voltage Electron microscope (SALVE) carries such a combined Cc/Cs corrector, optimized for voltages between 80 and 20 kV[8]. Even at 20 kV it resolves individual carbon atoms with a resolution better than 0.14 nm, over a wide field of view of 4096 × 4096 pixels. Between 40 kV (0.92 Å) and 80 kV (0.76 Å) the resolution is below one ångström, and for the same electron dose the contrast is higher[9]. How the corrector was built and first tested is told in the news article SALVE Cc Correction Realized, whose 30 kV images of graphene and MoS2 with diffractograms up to the third and fourth order the review also shows; experiment and image calculation agree there in the line scans, as expected from the optimum contrast conditions worked out for 20 and 80 kV[10] (news article Optimum HRTEM Contrast). The earlier steps towards 20 kV are told in TEM at 20 kV.

The gain is plainest in single-shot images of single-layer graphene (Fig. 1). At 80 kV with Cc/Cs correction, the honeycomb stands out sharply, and its diffractogram shows reflections out to 71 pm. At the same voltage with Cs correction alone, the lattice is barely visible in the noise, and only the innermost reflections at 213 pm appear. At 30 kV the Cc/Cs-corrected image still resolves the honeycomb, with reflections out to 107 pm. The review regards the Cc/Cs-corrected technology for TEM as a major improvement on the current technology; the box below compares the two corrector types at 80 kV.

The insets of Fig. 1 make the comparison measurable. Each pair of bright spots in a diffractogram stands for one set of lattice planes, and the smaller their spacing, the farther out the spots lie. For graphene the spacings are 213 pm for the innermost spots, then 123, 107, 82 and 71 pm. A microscope that transfers the 71 pm spacing thus shows details about half as large as the 142 pm between neighbouring carbon atoms. The lower row of Fig. 1 enlarges the dashed squares of the upper one: at 80 kV with Cc/Cs correction every hexagon stands out in a single exposure, whereas with Cs correction alone the honeycomb can only be guessed in the noise. At 30 kV the spots still reach 107 pm.

▸ Comparison: Cc/Cs vs. Cs correction at 80 kV

Choosing the voltage
A tunable low voltage allows the optimal choice for each sample. It is a compromise between resolving power, which is higher at higher voltage, and knock-on damage. In addition, especially non-conducting materials suffer from ionization, which usually grows at lower voltage[9]. Careful sample preparation is then needed to reduce these effects. Three techniques from Ulm give good results: the production of clean surfaces[11] (news article Dry-Cleaning Graphene), sandwiching the radiation-sensitive material between two graphene layers[12] (news article MoS2 Encapsulated in Graphene), and replacing hydrogen by heavier deuterium[13] (news article Deuterium Extends Molecule Lifetime).

Two other projects give independent checks of the SALVE resolution at the same voltage: the chromatic-aberration corrected PICO microscope in Jülich, and the Cc/Cs corrector designed for the TEAM I microscope of the American TEAM project; both are set out in the box below.

▸ Validation: FEI Titan Themis SALVE at 80 kV vs. FEI Titan PICO and TEAM I at 80 kV

Challenges named by the authors
The choice of voltage remains a trade-off between resolution, knock-on damage and ionization, and appropriate sample preparation is crucial for reaching the voltage-dependent resolution limits. Ionization in particular grows at low voltage and hits non-conducting materials hardest[9], so a lower voltage alone does not protect every sample.

Outlook
With lower voltage, higher resolution and higher contrast, HRTEM can now deliver reliable information on pore size distributions in graphene and related materials and on their edge structures[8]. The wide field of view of 4096 × 4096 pixels makes the SALVE microscope also very useful for dynamic studies and manipulations at the atomic scale.

Two things make this practical for radiation-sensitive samples. Edges and pores, which change fastest under the beam, can be imaged at the voltage that suits them, down to 20 kV, without giving up atomic resolution[5],[8]. And where a single shot is too noisy, averaging several experimental images raises the signal-to-noise ratio, and the averaged image can be compared directly with a simulated one, as the review shows for graphene and MoS2 at 30 kV[10].

Resource:
Backes, C., Abdelkader, A. M., Alonso, C., Andrieux-Ledier, A., Arenal, R., Azpeitia, J., Balakrishnan, N., Banszerus, L., Barjon, J., Bartali, R., Bellani, S., Berger, C., Berger, R., Ortega, M. M. B., Bernard, C., Beton, P. H., Beyer, A., Bianco, A., Bøggild, P., Bonaccorso, F., Barin, G. B., Botas, C., Bueno, R. A., Carriazo, D., Castellanos-Gomez, A., Christian, M., Ciesielski, A., Ciuk, T., Cole, M. T., Coleman, J., Coletti, C., Crema, L., Cun, H., Dasler, D., De Fazio, D., Díez, N., Drieschner, S., Duesberg, G. S., Fasel, R., Feng, X., Fina, A., Forti, S., Galiotis, C., Garberoglio, G., García, J. M., Garrido, J. A., Gibertini, M., Gölzhäuser, A., Gómez, J., Greber, T., Hauke, F., Hemmi, A., Hernandez-Rodriguez, I., Hirsch, A., Hodge, S. A., Huttel, Y., Jepsen, P. U., Jimenez, I., Kaiser, U., Kaplas, T., Kim, H., Kis, A., Papagelis, K., Kostarelos, K., Krajewska, A., Lee, K., Li, C., Lipsanen, H., Liscio, A., Lohe, M. R., Loiseau, A., Lombardi, L., López, M. F., Martin, O., Martín, C., Martínez, L., Martin-Gago, J. A., Martínez, J. I., Marzari, N., Mayoral, Á., McManus, J., Melucci, M., Méndez, J., Merino, C., Merino, P., Meyer, A. P., Miniussi, E., Miseikis, V., Mishra, N., Morandi, V., Munuera, C., Muñoz, R., Nolan, H., Ortolani, L., Ott, A. K., Palacio, I., Palermo, V., Parthenios, J., Pasternak, I., Patane, A., Prato, M., Prevost, H., Prudkovskiy, V., Pugno, N., Rojo, T., Rossi, A., Ruffieux, P., Samorì, P., Schué, L., Setijadi, E., Seyller, T., Speranza, G., Stampfer, C., Stenger, I., Strupinski, W., Svirko, Y., Taioli, S., Teo, K. B. K., Testi, M., Tomarchio, F., Tortello, M., Treossi, E., Turchanin, A., Vazquez, E., Villaro, E., Whelan, P. R., Xia, Z., Yakimova, R., Yang, S., Yazdi, G. R., Yim, C., Yoon, D., Zhang, X., Zhuang, X., Colombo, L., Ferrari, A. C., & Garcia-Hernandez, M. (2020).
Production and processing of graphene and related materials.
2D Mater. 7(2), 022001.
https://doi.org/10.1088/2053-1583/ab1e0a

Download this news article as PDF – for reading on paper, taking notes or filing.

References
  1. Kotakoski, J., Krasheninnikov, A. V., Kaiser, U., Meyer, J. C. (2011). From Point Defects in Graphene to Two-Dimensional Amorphous Carbon. Phys. Rev. Lett., 106, 105505. https://doi.org/10.1103/PhysRevLett.106.105505

  2. Eder, F. R., Kotakoski, J., Kaiser, U., Meyer, J. C. (2014). A Journey From Order to Disorder — Atom by Atom Transformation From Graphene to a 2D Carbon Glass. Sci Rep, 4, 4060. https://doi.org/10.1038/srep04060

  3. Banhart, F. (1999). Irradiation Effects in Carbon Nanostructures. Rep. Prog. Phys., 62, 1181–1221. https://doi.org/10.1088/0034-4885/62/8/201

  4. Egerton, R., McLeod, R., Wang, F., Malac, M. (2010). Basic Questions Related to Electron-Induced Sputtering in the TEM. Ultramicroscopy, 110, 991–997. https://doi.org/10.1016/j.ultramic.2009.11.003

  5. Suenaga, K., Iizumi, Y., Okazaki, T. (2011). Single Atom Spectroscopy With Reduced Delocalization Effect Using a 30 kV-STEM. Eur. Phys. J. Appl. Phys., 54, 33508. https://doi.org/10.1051/epjap/2011100414

  6. Ricolleau, C., Nelayah, J., Oikawa, T., Kohno, Y., Braidy, N., Wang, G., Hue, F., Florea, L., Pierron Bohnes, V., Alloyeau, D. (2012). Performances of an 80–200 kV Microscope Employing a Cold-FEG and an Aberration-Corrected Objective Lens. Microscopy (Tokyo), 62, 283–293. https://doi.org/10.1093/jmicro/dfs072

  7. Krivanek, O. L., Ursin, J. P., Bacon, N. J., Corbin, G. J., Dellby, N., Hrncirik, P., Murfitt, M. F., Own, C. S., Szilagyi, Z. S. (2009). High-Energy-Resolution Monochromator for Aberration-Corrected Scanning Transmission Electron Microscopy/Electron Energy-Loss Spectroscopy. Phil. Trans. R. Soc. A., 367, 3683–3697. https://doi.org/10.1098/rsta.2009.0087

  8. Linck, M., Hartel, P., Uhlemann, S., Kahl, F., Müller, H., Zach, J., Haider, M., Niestadt, M., Bischoff, M., Biskupek, J., Lee, Z., Lehnert, T., Börrnert, F., Rose, H., Kaiser, U. (2016). Chromatic Aberration Correction for Atomic Resolution TEM Imaging From 20 to 80 kV. Phys. Rev. Lett., 117, 076101. https://doi.org/10.1103/PhysRevLett.117.076101

  9. Kaiser, U., Biskupek, J., Meyer, J., Leschner, J., Lechner, L., Rose, H., Stöger-Pollach, M., Khlobystov, A., Hartel, P., Müller, H., Haider, M., Eyhusen, S., Benner, G. (2011). Transmission Electron Microscopy at 20kV for Imaging and Spectroscopy. Ultramicroscopy, 111, 1239–1246. https://doi.org/10.1016/j.ultramic.2011.03.012

  10. Lee, Z., Meyer, J., Rose, H., Kaiser, U. (2012). Optimum HRTEM Image Contrast at 20 kV and 80 kV—Exemplified by Graphene. Ultramicroscopy, 112, 39–46. https://doi.org/10.1016/j.ultramic.2011.10.009

  11. Algara-Siller, G., Lehtinen, O., Turchanin, A., Kaiser, U. (2014). Dry-Cleaning of Graphene. Appl. Phys. Lett., 104, 153115. https://doi.org/10.1063/1.4871997

  12. Algara-Siller, G., Kurasch, S., Sedighi, M., Lehtinen, O., Kaiser, U. (2013). The Pristine Atomic Structure of MoS2 Monolayer Protected From Electron Radiation Damage by Graphene. Appl. Phys. Lett., 103, 203107. https://doi.org/10.1063/1.4830036

  13. Chamberlain, T. W., Biskupek, J., Skowron, S. T., Bayliss, P. A., Bichoutskaia, E., Kaiser, U., Khlobystov, A. N. (2015). Isotope Substitution Extends the Lifetime of Organic Molecules in Transmission Electron Microscopy. Small, 11, 622–629. https://doi.org/10.1002/smll.201402081

  14. Boothroyd, C., Moreno, M., Duchamp, M., Kovács, A., Monge, N., Morales, G., Barbero, C., Dunin-Borkowski, R. (2014). Atomic Resolution Imaging and Spectroscopy of Barium Atoms and Functional Groups on Graphene Oxide. Ultramicroscopy, 145, 66–73. https://doi.org/10.1016/j.ultramic.2014.03.004

  15. Haider, M., Müller, H., Uhlemann, S., Zach, J., Loebau, U., Hoeschen, R. (2008). Prerequisites for a Cc/Cs-Corrected Ultrahigh-Resolution TEM. Ultramicroscopy, 108, 167–178. https://doi.org/10.1016/j.ultramic.2007.07.007