3D Imaging of Graphene

August 30, 2018 – Researchers at Ulm University have measured how the SALVE microscope, corrected for chromatic and spherical aberration, images graphene at 80 and 20 kV: down to 78 pm at 80 kV, and at 20 kV atoms 140 pm apart and a single vacancy at the right focus. At 20 kV the depth of focus is only a few nanometers, so a single raw image shows height changes at the edge of a hole or across a tilted sheet. Until then, graphene edges and heights had been imaged only at 80 kV or more, with a monochromator or an image series, in Tsukuba, Berkeley and at FEI in Eindhoven; now this is also possible at 20 kV with high resolution.

A sheet of graphene is one atom thin, but it is not flat in every sense: atoms sit on top of it, its edges hold other elements, and two sheets lie a few hundred picometers apart. A transmission electron microscope sees all of this in projection, as if pressed into one plane. Until now, imaging graphene at its edges and in depth needed 80 kV or more and either a monochromator or a whole series of images: at AIST in Tsukuba a tilt series at 120 kV told a single sheet from a folded double sheet[1], in Berkeley the TEAM 0.5 microscope filmed the atoms at the edge of a hole[2], and at FEI in Eindhoven the height of atoms was reconstructed from a whole series of images at stepped focus[3]. At 20 kV with SALVE, a single raw image already resolves graphene atom by atom up to the edge of a hole (Fig. 1). The same microscope also shows single vacancies: at 20 kV a single missing carbon atom is resolved in a raw image, but only at the right focus. Felix Börrnert and Ute Kaiser at Ulm University have measured how the SALVE microscope, corrected for both chromatic and spherical aberration, images graphene at 80 and 20 kV. At 20 kV its depth of focus shrinks to a few nanometers. A single raw image then already shows when part of the sample lies at another height: the graphene lattice at the edge of a hole reverses its contrast after a slight drift along the beam, while a heavier atom at the edge stays bright. What needed 80 kV or more and a monochromator or an image series before is thus possible at 20 kV with a chromatic-aberration corrector, below the voltage at which the beam knocks out carbon atoms even at an edge. The focal-series reconstruction from Eindhoven needed nineteen exposures for its height map; here one exposure is enough to see a height change.

Two correctors for low voltage
Graphene and other light materials have to be imaged at low voltage. A beam electron that hits a carbon nucleus can knock the atom out of its place if it transfers enough energy, and for a carbon atom in perfect graphene this starts at about 80 kV when the beam falls perpendicular on the sheet[4]. At an edge or in a carbon chain the bonds are weaker, and the threshold drops to about 20 kV[5]. Other damage mechanisms add to this[6]. Lower voltage, however, used to cost resolution: even with correctors for the spherical aberration, true atomic resolution at low voltage is hard to reach[7], because the energy spread of the electrons together with the chromatic aberration of the lenses blurs the image. A monochromator narrows the energy spread[8], but it throws away most of the electrons, and it does nothing for electrons that lose energy in the sample.

The SALVE instrument in Ulm solves this with a corrector for the chromatic aberration as well[9] (see SALVE Cc Correction Realized[10]). Its resolution is no longer limited by the energy spread but by the thermal magnetic noise in the corrector, the so-called Johnson–Nyquist noise[11]. With it, Börrnert and Kaiser recorded graphene at the upper and lower ends of its voltage range, 80 and 20 kV, and calculated for each image how the microscope transfers contrast.

How much simpler this makes the work shows in a comparison with three earlier studies at 120 and 80 kV, set out in the validation boxes further below. The Tsukuba study needed 120 kV, sequences of 20–40 frames and a tilt of 20° to tell one layer from two. The Berkeley movie needed a monochromator and one image per frame, 110 frames in all, and gave no height. The Eindhoven reconstruction needed a monochromator, 19 images at focus steps of 1.7 nm and 2.2 × 107 e−/nm2 for the series, and the edge had to be left out because it changed during the recording. SALVE at 20 kV needs one raw image with 8.5 × 106 e−/nm2, without monochromator and without processing. Where the calculation and the images can be compared, they agree: 75 pm calculated against signals up to 71 pm at 80 kV, 130 pm against atoms 140 pm apart at 20 kV, and 5.3 nm against 5.2 nm of focus between two contrast maxima. The box below lists the microscope and the settings and shows the raw images of graphene at 80 kV (Fig. 2) and 20 kV (Fig. 3).

▸ Instruments and samples

The box below explains why a vacancy at 20 kV shows at only one of three foci (Fig. 4) and describes the distorted vacancy at 80 kV (Fig. 5).

▸ Single vacancies at 80 and 20 kV

An edge at two heights
Two images of the same hole in graphene, taken 40 s apart at 20 kV, show how sensitive the image is to height (Fig. 6). The sample drifted slightly along the beam between them, and the graphene lattice turned from bright atoms to dark atoms. A heavier atom bound to the edge of the hole stayed bright in both: for elements heavier than carbon the weak-phase-object picture breaks down at such low electron energies. The edges also show fringes reaching into the vacuum, wider in the first image than in the second. Calculated for the neighboring transfer bands, 6 nm and 11 nm of defocus give 0.6 nm and 0.4 nm of delocalization, which matches the width of the fringes. Between the two exposures the sample received 8.5 × 107 e−/nm2, and the hole grew by about 0.5 nm in every direction, roughly one unit cell per edge per 108 e−/nm2.

The same kind of drift had been seen before at 80 kV. When researchers from UC Berkeley and the Lawrence Berkeley National Laboratory filmed the edge of a hole in graphene on the monochromated TEAM 0.5, every edge atom was resolved, but small drifts of the suspended sheet along the beam moved it out of the focal plane, and the focus had to be readjusted during the series[2]. At 80 kV the edge atoms were also knocked out, and the hole grew on a time scale of minutes[2]. At 20 kV with the chromatic aberration corrected, the drift itself becomes the signal: the contrast reversal shows that the sheet has moved by a few nanometers, without refocusing. Beam damage is not directly comparable, since dose rates and exposure differ, but at 20 kV the hole grew by only about one unit cell per edge per 108 e−/nm2.

The box below compares the depth of focus of SALVE at 20 kV, described in the instrument box, with three earlier approaches: a tilt series of folded graphene edges at 120 kV from Tsukuba, and at 80 kV with a monochromator the movie of a graphene edge from Berkeley and a reconstruction from Eindhoven that measures the height of single atoms in a bilayer, at much greater effort.

▸ Validation: JEM-2010F at 120 kV, TEAM 0.5 and FEI Titan G2 at 80 kV vs. SALVE at 20 kV

How well the calculated transfer describes the images is checked in a second box, which also shows the two tilted sheets (Fig. 7).

▸ Validation: contrast-transfer calculation vs. images

Room to tilt
The authors also put their numbers into perspective. Nonlinear signals often make microscopes look sharper than they are: a Titan without monochromator has an information limit of 190 pm at 80 kV[7], yet 120 pm was often reported because of the second-order graphene spots. Monochromators reach a similar focus spread as a chromatic corrector only by cutting away most of the electrons, and inelastically scattered electrons are then lost and add noise, while with the corrector the whole current of the source forms the image. Another route, very narrow pole-piece gaps[17], halves the aberrations but leaves almost no room for the sample: holders must be extra flat and tilting is severely limited. SALVE keeps a standard gap of 5.4 mm, into which every commercial in-situ holder fits.

Challenges named by the authors
The residual fifth-order spherical aberration brings back contrast oscillations and delocalization at 20 kV, which is why the point resolution of 150 pm trails the information limit. The Lentzen focus demands a precision of about 1 nm, and near zero defocus it cannot be found from Thon rings, since a corrected microscope shows none; it has to be set by maximizing the atom contrast while no Thon rings appear in the amorphous residues. At 20 kV the illumination semi-angle grows, and so does the illumination damping, which may matter for modes that rely on spatial coherence, such as holography. The images also had to be strongly oversampled, more than eight times at 20 kV, to overcome the limited dynamic range of the camera, and even at 20 kV the beam slowly enlarged a hole in the graphene.

Outlook
At 80 kV SALVE resolves graphene down to 78 pm and shows the Jahn–Teller distortion of a single vacancy, and at 20 kV, close to the knock-on threshold even of edge atoms, it still separates atoms 140 pm apart and resolves a single vacancy at the right focus. Its depth of focus of a few nanometers turns every image into a coarse map of height, and its wide pole-piece gap leaves room to tilt and to work in situ. The approach using chromatic-aberration correction in addition to geometric-aberration correction in low-voltage TEM “is greatly beneficial for in situ imaging with atomic resolution,” the authors conclude. The work was part of the SALVE project at Ulm University, funded by the DFG and the Ministry of Science, Research and the Arts of Baden-Württemberg.

Resource:
Börrnert, F., & Kaiser, U. (2018).
Chromatic- and geometric-aberration-corrected TEM imaging at 80 kV and 20 kV.
Phys. Rev. A 98(2), 023861.
https://doi.org/10.1103/PhysRevA.98.023861

Update – February 10, 2019

The news article of August 30, 2018 ends above. Later work that builds on it is listed below.

Half a year later, Zhongbo Lee, Tibor Lehnert, Ute Kaiser and Harald Rose at Ulm University tested how simple an image simulation may be once the chromatic aberration is corrected[18]. They compared three models of partial coherence, from the full incoherent summation to the quick quasi-coherent model, with focal series of MoTe2 monolayers and bilayers, 0.36 and about 1 nm thick, recorded at 80 kV on the Cs-corrected FEI Titan 80-300 and on the Cc/Cs-corrected SALVE instrument. With the Cc corrector the residual focal spread is only about 0.5 nm instead of about 4 nm, and all three models reproduce the images of both the monolayer and the bilayer. Calculated for thicker MoTe2, up to twenty layers or 14 nm, the quick model still gives at least 0.79 of the atom intensity of the full calculation; with Cs correction alone the ratio stays below 0.8 and falls toward 0.1 above about 6.6 nm, so the costly calculation is needed. For samples several nanometers deep, correcting the chromatic aberration thus simplifies not only the imaging but also its interpretation.

Download this news article as PDF – for reading on paper, taking notes or filing.

References
  1. Liu, Z., Suenaga, K., Harris, P. J. F., Iijima, S. (2009). Open and Closed Edges of Graphene Layers. Phys. Rev. Lett., 102, 015501. https://doi.org/10.1103/PhysRevLett.102.015501

  2. Girit, Ç. Ö., Meyer, J. C., Erni, R., Rossell, M. D., Kisielowski, C., Yang, L., Park, C.-H., Crommie, M. F., Cohen, M. L., Louie, S. G., Zettl, A. (2009). Graphene at the Edge: Stability and Dynamics. Science, 323, 1701–1705. https://doi.org/10.1126/science.1166862

  3. Jinschek, J. R., Yucelen, E., Calderon, H. A., Freitag, B. (2011). Quantitative Atomic 3-D Imaging of Single/Double Sheet Graphene Structure. Carbon, 49, 556–562 (available online 28 October 2010). https://doi.org/10.1016/j.carbon.2010.09.058

  4. Meyer, J. C., Eder, F., Kurasch, S., Skakalova, V., Kotakoski, J., Park, H. J., Roth, S., Chuvilin, A., Eyhusen, S., Benner, G., et al. (2012). Accurate Measurement of Electron Beam Induced Displacement Cross Sections for Single-Layer Graphene. Phys. Rev. Lett., 108, 196102. https://doi.org/10.1103/PhysRevLett.108.196102

  5. Bell, D. C., Russo, C. J., Kolmykov, D. V. (2012). 40keV Atomic Resolution TEM. Ultramicroscopy, 114, 31–37. https://doi.org/10.1016/j.ultramic.2011.12.001

  6. Banhart, F. (1999). Irradiation Effects in Carbon Nanostructures. Rep. Prog. Phys., 62, 1181–1221. https://doi.org/10.1088/0034-4885/62/8/201

  7. Barthel, J., Thust, A. (2008). Quantification of the Information Limit of Transmission Electron Microscopes. Phys. Rev. Lett., 101, 200801. https://doi.org/10.1103/PhysRevLett.101.200801

  8. Freitag, B., Kujawa, S., Mul, P. M., Ringnalda, J., Tiemeijer, P. C. (2005). Breaking the Spherical and Chromatic Aberration Barrier in Transmission Electron Microscopy. Ultramicroscopy, 102, 209–214. https://doi.org/10.1016/j.ultramic.2004.09.013

  9. Linck, M., Hartel, P., Uhlemann, S., Kahl, F., Müller, H., Zach, J., Haider, M., Niestadt, M., Bischoff, M., Biskupek, J., et al. (2016). Chromatic Aberration Correction for Atomic Resolution TEM Imaging From 20 to 80 kV. Phys. Rev. Lett., 117, 076101. https://doi.org/10.1103/PhysRevLett.117.076101

  10. SALVE news (2016). SALVE Cc Correction Realized. salve-project.de, August 9, 2016. https://www.salve-project.de/newspress/SALVE-CC-correction-realized.html

  11. Uhlemann, S., Müller, H., Hartel, P., Zach, J., Haider, M. (2013). Thermal Magnetic Field Noise Limits Resolution in Transmission Electron Microscopy. Phys. Rev. Lett., 111, 046101. https://doi.org/10.1103/PhysRevLett.111.046101

  12. Börrnert, F., Renner, J., Kaiser, U. (2018). Electron Source Brightness and Illumination Semi-Angle Distribution Measurement in a Transmission Electron Microscope. Microsc. Microanal., 24, 249–255. https://doi.org/10.1017/S1431927618000223

  13. Lentzen, M., Jahnen, B., Jia, C. L., Thust, A., Tillmann, K., Urban, K. (2002). High-Resolution Imaging With an Aberration-Corrected Transmission Electron Microscope. Ultramicroscopy, 92, 233–242. https://doi.org/10.1016/S0304-3991(02)00139-0

  14. Haider, M., Hartel, P., Müller, H., Uhlemann, S., Zach, J. (2010). Information Transfer in a TEM Corrected for Spherical and Chromatic Aberration. Microsc. Microanal., 16, 393–408. https://doi.org/10.1017/S1431927610013498

  15. El-Barbary, A. A., Telling, R. H., Ewels, C. P., Heggie, M. I., Briddon, P. R. (2003). Structure and Energetics of the Vacancy in Graphite. Phys. Rev. B, 68, 144107. https://doi.org/10.1103/PhysRevB.68.144107

  16. Lee, Z., Hambach, R., Kaiser, U., Rose, H. (2017). Significance of Matrix Diagonalization in Modelling Inelastic Electron Scattering. Ultramicroscopy, 175, 58–66. https://doi.org/10.1016/j.ultramic.2016.11.011

  17. Morishita, S., Mukai, M., Suenaga, K., Sawada, H. (2016). Resolution Enhancement in Transmission Electron Microscopy With 60-kV Monochromated Electron Source. Appl. Phys. Lett., 108, 013107. https://doi.org/10.1063/1.4939653

  18. Lee, Z., Lehnert, T., Kaiser, U., Rose, H. (2019). Comparison of Different Imaging Models Handling Partial Coherence for Aberration-Corrected HRTEM at 40–80 kV. Ultramicroscopy, 203, 68–75. https://doi.org/10.1016/j.ultramic.2019.01.007